Crevice Corrosion in a Subsea System — Aspect Before Analysis

15 images

M

Material

79 classified

Browse all Material →
P

Product

96 classified

Browse all Product →
Ap

Application

37 classified

Browse all Application →
C

Condition

84 classified

Browse all Condition →
Cm

Capture method

52 classified

Browse all Capture method →
Df

Detail focus

208 classified

Browse all Detail focus →

Sharpest next filters

Browse by category (2)
Microstructure73
+65 more

and 25 more not shown here — refine in the Atlas

Standard298
+290 more

and 250 more not shown here — refine in the Atlas

15 images
ML00178 / Jan.2022
Cold cracks in Cr-Mo Welded Forging
M - CrMo SteelP - ForgingAp - O&G Well DrillingCd - Welding Defect
Cm - Nital Etched Micrography by SEMDf - Cold cracking
ML00173 / May.2021
Welding Cracks in an Aged HP Cast Fitting
M - Heat Resistant SteelP - Cast FtittingAp - PetrochemicalCd - Welding
Cm - Kalling Etched Micrography by OMDf - Hot cracking
ML00162 / Apr.2020
Valve Body Crack Growth from Weld Defects
M - Low Alloy Medium Carbon QTP - Valve BodyAp - O&G Well DrillingCd - Fatigue Induced by a Defect
Cm - NItal Etched MacroDf - Hot cracking
ML00150 / Dec.2018
Vibration Induced Fatigue in a SS Oil Piping
M - Duplex Stainless SteelP - PipingAp - FPSOCd - Vibration Induced Fatigue
Cm - NaOH Electrolytic Etched MicroDf - Lack of fusion
Micrography of the welded joint, at the root, presenting hot cracks.  The imposed high energy in the root due to the ceramic backing support created a condition for cracking.
1100
ML00118 / Jan.2018
Non qualified GMAW of Aluminum Plates
M - Aluminum Magnesium ManganeseP - Welded Testpiece for QualificationAp - ShipCd - Non qualified
Cm - Keller Etched Micrography by OMDf - Hot cracking

More from these cases

ML00178 — Cold cracks in Cr-Mo Welded ForgingM - CrMo SteelP - ForgingAp - O&G Well DrillingCd - Welding Defect
ML00178 / Jan.2022
Cold cracks in Cr-Mo Welded Forging
M - CrMo SteelP - ForgingAp - O&G Well DrillingCd - Welding Defect
Cm - Nital Etched Micrography by SEMDf - Cold cracking
ML00178 / Jan.2022
Cold cracks in Cr-Mo Welded Forging
M - CrMo SteelP - ForgingAp - O&G Well DrillingCd - Welding Defect
Cm - Nital Etched Micrography by SEMDf - Cold cracking
ML00162 — Valve Body Crack Growth from Weld DefectsM - Low Alloy Medium Carbon QTP - Valve BodyAp - O&G Well DrillingCd - Fatigue Induced by a Defect
ML00162 / Apr.2020
Valve Body Crack Growth from Weld Defects
M - Low Alloy Medium Carbon QTP - Valve BodyAp - O&G Well DrillingCd - Fatigue Induced by a Defect
Cm - As polished micrographyDf - Hot cracking
ML00162 / Apr.2020
Valve Body Crack Growth from Weld Defects
M - Low Alloy Medium Carbon QTP - Valve BodyAp - O&G Well DrillingCd - Fatigue Induced by a Defect
Cm - As polished micrographyDf - Hot cracking
ML00162 / Apr.2020
Valve Body Crack Growth from Weld Defects
M - Low Alloy Medium Carbon QTP - Valve BodyAp - O&G Well DrillingCd - Fatigue Induced by a Defect
Cm - As polished micrographyDf - Hot cracking
ML00162 / Apr.2020
Valve Body Crack Growth from Weld Defects
M - Low Alloy Medium Carbon QTP - Valve BodyAp - O&G Well DrillingCd - Fatigue Induced by a Defect
Cm - Nital Etched Micrography by OMDf - Hot cracking
ML00162 / Apr.2020
Valve Body Crack Growth from Weld Defects
M - Low Alloy Medium Carbon QTP - Valve BodyAp - O&G Well DrillingCd - Fatigue Induced by a Defect
Cm - As polished micrographyDf - Hot cracking
ML00150 — Vibration Induced Fatigue in a SS Oil PipingM - Duplex Stainless SteelP - PipingAp - FPSOCd - Vibration Induced Fatigue
ML00150 / Dec.2018
Vibration Induced Fatigue in a SS Oil Piping
M - Duplex Stainless SteelP - PipingAp - FPSOCd - Vibration Induced Fatigue
Cm - NaOH Electrolytic Etched MicroDf - Lack of fusion
ML00118 — Non qualified GMAW of Aluminum PlatesM - Aluminum Magnesium ManganeseP - Welded Testpiece for QualificationAp - ShipCd - Non qualified
Micrography of the welded joint, at the root, showing hot cracks with intergranular morphology.
146
ML00118 / Jan.2018
Non qualified GMAW of Aluminum Plates
M - Aluminum Magnesium ManganeseP - Welded Testpiece for QualificationAp - ShipCd - Non qualified
Cm - Keller Etched Micrography by OMDf - Hot cracking
Micrographic detail of the welded joint, at the root, presenting hot cracks.  The presence of these defects were responsible for reducing the material strenght (rupturing in lower strenght than the requirements) and ductility (cracking in bending tests).
116
ML00118 / Jan.2018
Non qualified GMAW of Aluminum Plates
M - Aluminum Magnesium ManganeseP - Welded Testpiece for QualificationAp - ShipCd - Non qualified
Cm - Keller Etched Micrography by OMDf - Hot cracking

most recent

The location of the threaded fitting started leaking after less than five years in service. 
Although the corrosion rate was not high, the localized material loss in the threaded surface of the carbon steel flange allowed the connection leakage.
769
ML00184 / Apr.2023
Dissimilar Steels in a Threaded Connection
M - Low Carbon SteelP - ForgingAp - OffshoreCd - Localized Dissolution
Cm - Aspect Before AnalysisDf - General View
Front wheel 17 x 7J of a passenger vehicle (identified as WHEEL 1) that broke during a car accident on a road.
1644
ML00183 / Dec.2022
Ductile Behavior of an Aluminum Wheel
M - Aluminum Silicon MagnesiumP - CastingAp - AutomotiveCd - Ductile Behavior
Cm - Aspect Before AnalysisDf - General View
Tool fixture 5" long, nominal diameter 2", presenting a recess 1/2" deep from two sides.  The rupture occurred about 2" from the end of the rod.   Scale in milimeters.
523
ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Aspect Before AnalysisDf - General View
Pinion of hypoid gearbox, assembled in a 1560-mm long shaft that operated during more than 60,000 hours, and removed from service due to unacceptable wear damage.
1028
ML00181 / Apr.2022
Wear of a Carburized Hypoid Gear
M - Low Alloy for Thermochemical TreatmentP - Pinion-crown assemblyAp - ShipCd - Wear
Cm - Aspect Before AnalysisDf - General View
Aspect of the 3 1/2" diameter tube after the water leakage in high temperature.
962
ML00180 / Mar.2022
Local Melting of Copper Cooling Tubes
M - Pure CopperP - Cooling TubeAp - SiderurgyCd - Overheating
Cm - Aspect Before AnalysisDf - General View
2" drain line from the main 10" line. The leakage occurred at the margin of the weld, a short time after the introduction of the reinforced ribs to reduce vibration.
641
ML00179 / Feb.2022
Hydrides in Titanium Weld
M - Unalloyed TitaniumP - In Field WeldAp - Chemical IndustryCd - Hydride Formation
Cm - Field photoDf - General View
The drilling connector, 21" diameter, presented a crack at the margin of the weld in the forging side (left side of the weld in the figure).
745
ML00178 / Jan.2022
Cold cracks in Cr-Mo Welded Forging
M - CrMo SteelP - ForgingAp - O&G Well DrillingCd - Welding Defect
Cm - Aspect Before AnalysisDf - General View
Macrography of the longitudinally seam weld of the 24" diameter tube, showing that it was welded from both sides and there is a segregation line in the center of the tube thickness.
737
ML00177 / Dec.2021
Cr-Mo Seam Welded Tube
M - CrMo SteelP - Longitudinally Seam WeldedAp - Fired HeaterCd - Not according to spec
Cm - NItal Etched MacroDf - Seam
The titanium rotor blade of a flowmeter broke after two years in service in an acid environment, containing H2S.
339
ML00176 / Nov.2021
Hydride Formation in a Titanium Blade
M - Unalloyed TitaniumP - BladeAp - Oil and GasCd - Hydride Formation
Cm - Aspect Before AnalysisDf - General View
Aspect of the wire rope, 1 1/2" diameter, presenting regions of flattened  areas at the surface of the outer wires. It is a 6 x 19 Seale construction, right regular lay.
552
ML00175 / Aug.2021
Localized External Wear of a Wire Rope
M - High Carbon SteelP - Wire RopeAp - Oil and GasCd - Wear
Cm - Aspect Before AnalysisDf - General View
The carcass was manufactured using niobium stabilized plates, grade AISI 347, with circumferential welds, where the through wall cracks were detected.
300
ML00174 / Jul.2021
Carburization of a 347 SS Welded Joint
M - Austenitic Stainless SteelP - Fabrication WeldAp - EnergyCd - Carburization
Cm - Field photoDf - General View
Aged microstructure of the HP stainless steel, modified with 1%Nb, cast fitting, tubular, operating for 6 years in a furnace which design temperature is 1100°C.  The material presented a network of primary carbides, white and grey, and an austenitic matrix with coalescing secondary precipitation. Some voids. The Vickers identation indicates a hardness value about 260HV 100g in the aged austenitic matrix.
492
ML00173 / May.2021
Welding Cracks in an Aged HP Cast Fitting
M - Heat Resistant SteelP - Cast FtittingAp - PetrochemicalCd - Welding
Cm - Kalling Etched Micrography by OMDf - Microhardness identations
TECMETAL