Ferrite and Pearlite
27 cases · 58 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00171 / Feb.2021
Corrosion Fatigue of U Bolt Pipe Clamp
M - Low Carbon SteelP - BoltAp - ShipCd - Corrosion Fatigue
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite

ML00163 / Jun.2020
Corrosion Fatigue of a Boiler Waterwall Tube
M - Low Carbon SteelP - Seamless tubeAp - BoilerCd - Corrosion Fatigue
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite

ML00154 / Jan.2019
High Strength Cast Iron Crankshaft
M - Nodular Cast IronP - CastingAp - EngineCd - Surface treatment
Cm - Nital Etched Micrography by SEMDf - Ferrite and Pearlite

ML00149 / Dec.2018
Vibration Induced Fatigue in a Gas Piping
M - Low Carbon SteelP - Piping spoolAp - FPSOCd - Vibration Induced Fatigue
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite

ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite

ML00141 / Jul.2018
Brittle Fracture of a Corroded Gray Cast Iron
M - Gray Cast ironP - CastingAp - EngineCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite

ML00140 / May.2019
Preferential Corrosion of Pipe Seam Weld
M - Low Carbon SteelP - Longitudinal Seam Welded PipeAp - ShipCd - Preferential Dissolution
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite

ML00128 / Apr.2018
MIC of a Stored Hydraulic Cylinder
M - Low Carbon SteelP - Chromium PlatedAp - OffshoreCd - Localized Dissolution
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite
More from these cases

ML00171 / Feb.2021
Corrosion Fatigue of U Bolt Pipe Clamp
M - Low Carbon SteelP - BoltAp - ShipCd - Corrosion Fatigue
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite

ML00149 / Dec.2018
Vibration Induced Fatigue in a Gas Piping
M - Low Carbon SteelP - Piping spoolAp - FPSOCd - Vibration Induced Fatigue
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite

ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite

ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite

ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite

ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - Nital Etched Micrography by SEMDf - Ferrite and Pearlite

ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - Nital Etched Micrography by SEMDf - Ferrite and Pearlite

ML00140 / May.2019
Preferential Corrosion of Pipe Seam Weld
M - Low Carbon SteelP - Longitudinal Seam Welded PipeAp - ShipCd - Preferential Dissolution
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite

ML00128 / Apr.2018
MIC of a Stored Hydraulic Cylinder
M - Low Carbon SteelP - Chromium PlatedAp - OffshoreCd - Localized Dissolution
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite