Crevice Corrosion in a Subsea System — Aspect Before Analysis

Throught wall cracking of the waterwall tube at the leakage position, thick edged,  The external surface of the tube was grounded to remove the membrane and the cracking is associated to the tube attachement.
242
ML00163 / Jun.2020
Corrosion Fatigue of a Boiler Waterwall Tube
M - Low Carbon SteelP - Seamless tubeAp - BoilerCd - Corrosion Fatigue
Cm - Transverse Section AspectDf - Thick-edged rupture