Crevice Corrosion in a Subsea System — Aspect Before Analysis

102 images

M

Material

79 classified

Browse all Material →
P

Product

96 classified

Browse all Product →
Ap

Application

37 classified

Browse all Application →
C

Condition

84 classified

Browse all Condition →
Cm

Capture method

52 classified

Browse all Capture method →
Df

Detail focus

208 classified

Browse all Detail focus →

Sharpest next filters

Browse by category (2)
102 images
Aspect of the stub end, that is used in combination with a lap joint flange.  In this case it was prepared from a seam welded pipe, longitudinal, also with circunferential weld to the stub face (which means it was not flared).  The cracking is circunferential in the non painted region, not associated to any welded area.
435
ML00168 / Aug.2020
SCC of Austenitic SS Flange Stub End
M - Austenitic Stainless SteelP - Stub EndAp - Chemical IndustryCd - Stress Corrosion
Cm - Aspect Before AnalysisDf - General View
Aspect "as received" of the seamless tube at the curved position, showing the longitudinal crack and corrosion products at the tube surface.
836
ML00165 / Jul.2020
SCC of Aluminum Bronze Heating Coil
M - Aluminum BronzeP - Seamless tubeAp - Oil and GasCd - Stress Corrosion
Cm - Aspect Before AnalysisDf - General View
Optical micrography of a longitudinal section of the fractured bolt, at the thread.  The material is austenitic, free from carbides, and the threads were almost removed by the stress corrosion cracks.
756
ML00157 / Feb.2020
Bolts Under Chloride SCC Conditions
M - Austenitic Stainless SteelP - BoltAp - Oil and GasCd - Stress Corrosion
Cm - Oxalic Acid Electrolytic EtchDf - Stress Corrosion Cracks
The macrography of a longitudinal section of the shell plate (sample removed from the boiler), at the position of the fillet weld (sealing weld) with a tube, where surface welding repairs created conditions for cracking the base material in a transgranular morphology. Several cracks were identify starting from the steam drum internal surface.
448
ML00019 / Apr.2017
Transgranular SCC in Boiler Steam Drum
M - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Transverse Section AspectDf - Cracks
Aspect of the heat exchanger plate showing the rupture of the plate in multiple cracks, starting at the side of the crude oil with high salinity.
727
ML00051 / Apr.2020
Chloride SCC of 316 Heat Exchanger Plate
M - Austenitic Stainless SteelP - Heat Exchanger PartAp - FPSOCd - Stress Corrosion
Cm - Aspect Before AnalysisDf - Cracking
Typical branched stress corrosion cracks in a low carbon steel, ferritic-pertlitic structure. The cracks are filled with corrosion products.
771
ML00018 / Apr.2017
SCC in Boiler Steam Drum
M - Low Carbon SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Branched Cracks
Steam drum presenting cracks in the shell, connecting tube holes.
1704
ML00020 / Apr.2017
Intergranular SCC in Boiler Steam Drum Repair
M - Low Carbon SteelP - Repair WeldAp - BoilerCd - Stress Corrosion
Cm - Aspect Before AnalysisDf - Cracking
Regions of the pin thread presenting pitting corrosion.
635
ML00016 / Apr.2017
SCC in Free Cutting 303SS
M - Austenitic Stainless SteelP - Machined PartAp - OffshoreCd - Stress Corrosion
Cm - Surface Aspect by SEMDf - Localized Corrosion

More from these cases

ML00168 — SCC of Austenitic SS Flange Stub EndM - Austenitic Stainless SteelP - Stub EndAp - Chemical IndustryCd - Stress Corrosion
ML00168 / Aug.2020
SCC of Austenitic SS Flange Stub End
M - Austenitic Stainless SteelP - Stub EndAp - Chemical IndustryCd - Stress Corrosion
Cm - Aspect Before AnalysisDf - Cracking
ML00168 / Aug.2020
SCC of Austenitic SS Flange Stub End
M - Austenitic Stainless SteelP - Stub EndAp - Chemical IndustryCd - Stress Corrosion
Cm - Oxalic Acid Electrolytic EtchDf - Longitudinal Section
ML00168 / Aug.2020
SCC of Austenitic SS Flange Stub End
M - Austenitic Stainless SteelP - Stub EndAp - Chemical IndustryCd - Stress Corrosion
Cm - Oxalic Acid Electrolytic EtchDf - Austenite
ML00168 / Aug.2020
SCC of Austenitic SS Flange Stub End
M - Austenitic Stainless SteelP - Stub EndAp - Chemical IndustryCd - Stress Corrosion
Cm - Oxalic Acid Electrolytic EtchDf - Austenite
ML00168 / Aug.2020
SCC of Austenitic SS Flange Stub End
M - Austenitic Stainless SteelP - Stub EndAp - Chemical IndustryCd - Stress Corrosion
Cm - Longitudinal Section AspectDf - Multiple cracks

+10 more from this case →

ML00165 — SCC of Aluminum Bronze Heating CoilM - Aluminum BronzeP - Seamless tubeAp - Oil and GasCd - Stress Corrosion
Aspect of the external tube surface after cleaning. It is possible to see that the cracks are longitudinal to the tube and localized in positions where the surface is corroded.
132
ML00165 / Jul.2020
SCC of Aluminum Bronze Heating Coil
M - Aluminum BronzeP - Seamless tubeAp - Oil and GasCd - Stress Corrosion
Cm - Surface AspectDf - External Surface
Aspect of the internal tube surface after a longitudinal cut, without cleaning.  It is possible to see a clean surface inside the tube.
104
ML00165 / Jul.2020
SCC of Aluminum Bronze Heating Coil
M - Aluminum BronzeP - Seamless tubeAp - Oil and GasCd - Stress Corrosion
Cm - Surface AspectDf - Internal Surface
Micrography of the tranverse section of the tube, in the center of the thickness.  There are small grains and large grains, characterizing a dual grain size.  The large grains size is about 100 microns, more than 10 times larger than the average size of the smaller grains size.
101
ML00165 / Jul.2020
SCC of Aluminum Bronze Heating Coil
M - Aluminum BronzeP - Seamless tubeAp - Oil and GasCd - Stress Corrosion
Cm - FeCl3+HCl+H2O Etched MicroDf - Dual grain sizes
ML00165 / Jul.2020
SCC of Aluminum Bronze Heating Coil
M - Aluminum BronzeP - Seamless tubeAp - Oil and GasCd - Stress Corrosion
Cm - FeCl3+HCl+H2O Etched MicroDf - Alpha
ML00165 / Jul.2020
SCC of Aluminum Bronze Heating Coil
M - Aluminum BronzeP - Seamless tubeAp - Oil and GasCd - Stress Corrosion
Cm - As polished micrographyDf - Cracking

+12 more from this case →

ML00157 — Bolts Under Chloride SCC ConditionsM - Austenitic Stainless SteelP - BoltAp - Oil and GasCd - Stress Corrosion
Aspect of a 5/16" bolt manufactured in an AISI 316 austenitic stainless steel, that was also operating inside the pressure vessel, but was not yet damaged.  It is a hexagonal head bolt, 1 1/2" long, fastened with a hexagonal nut and a lock washer.
118
ML00157 / Feb.2020
Bolts Under Chloride SCC Conditions
M - Austenitic Stainless SteelP - BoltAp - Oil and GasCd - Stress Corrosion
Cm - Aspect Before AnalysisDf - General View
Low magnification micrography, by optical microscope, of the longitudinal section of a damaged bolt, in the center of the thickness. The microstructure is austenitic, free from carbides.
100
ML00157 / Feb.2020
Bolts Under Chloride SCC Conditions
M - Austenitic Stainless SteelP - BoltAp - Oil and GasCd - Stress Corrosion
Cm - Oxalic Acid Electrolytic EtchDf - Austenite
ML00157 / Feb.2020
Bolts Under Chloride SCC Conditions
M - Austenitic Stainless SteelP - BoltAp - Oil and GasCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Strain Hardened
ML00157 / Feb.2020
Bolts Under Chloride SCC Conditions
M - Austenitic Stainless SteelP - BoltAp - Oil and GasCd - Stress Corrosion
Cm - Oxalic Acid Electrolytic EtchDf - Strain Hardened
ML00157 / Feb.2020
Bolts Under Chloride SCC Conditions
M - Austenitic Stainless SteelP - BoltAp - Oil and GasCd - Stress Corrosion
Cm - Aspect Before AnalysisDf - Fracture

+8 more from this case →

ML00019 — Transgranular SCC in Boiler Steam DrumM - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Schematic drawing presenting the longitudinal section of the shell plate (sample removed from the boiler), at the position of the fillet weld (sealing weld) with a tube,  where surface welding repairs created conditions for cracking the base material in a transgranular morphology. Several cracks were identify starting from the steam drum internal surface.
120
ML00019 / Apr.2017
Transgranular SCC in Boiler Steam Drum
M - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Identification drawingDf - Cracks
Micrography of a transverse section of the shell plate in a cracked position showing the transgranular morphology of the stress corrosion cracks.
167
ML00019 / Apr.2017
Transgranular SCC in Boiler Steam Drum
M - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by SEMDf - Transgranular Cracking
ML00019 / Apr.2017
Transgranular SCC in Boiler Steam Drum
M - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite
ML00019 / Apr.2017
Transgranular SCC in Boiler Steam Drum
M - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite
ML00019 / Apr.2017
Transgranular SCC in Boiler Steam Drum
M - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Branched Cracks

+4 more from this case →

ML00051 — Chloride SCC of 316 Heat Exchanger PlateM - Austenitic Stainless SteelP - Heat Exchanger PartAp - FPSOCd - Stress Corrosion
Macrography of the surface of the cracked heat exchanger plate, manufactured in austenitic stainless steel.
159
ML00051 / Apr.2020
Chloride SCC of 316 Heat Exchanger Plate
M - Austenitic Stainless SteelP - Heat Exchanger PartAp - FPSOCd - Stress Corrosion
Cm - Macro Oxalic Acid Electrolytic EtchedDf - Cracking
Micrography of the plate material presenting a granular austenitic structure, free from precipitation.
122
ML00051 / Apr.2020
Chloride SCC of 316 Heat Exchanger Plate
M - Austenitic Stainless SteelP - Heat Exchanger PartAp - FPSOCd - Stress Corrosion
Cm - Eletrolytically Etched Micrography by OMDf - Austenite
Micrographic detail of the austenitic microstructure of the heat exchanger plate, free from carbides that suggest the adoption of a material in a solution annealed condition, although the high hardness level indicates cold working.
109
ML00051 / Apr.2020
Chloride SCC of 316 Heat Exchanger Plate
M - Austenitic Stainless SteelP - Heat Exchanger PartAp - FPSOCd - Stress Corrosion
Cm - Eletrolytically Etched Micrography by OMDf - Austenite
Micrography presenting the transgranular morphology of the stress corrosion cracks of the austenitic plate.  EDS analysis at the plate surface indicated high Cl peaks.
111
ML00051 / Apr.2020
Chloride SCC of 316 Heat Exchanger Plate
M - Austenitic Stainless SteelP - Heat Exchanger PartAp - FPSOCd - Stress Corrosion
Cm - Eletrolytically Etched Micrography by OMDf - Corrosion Cracking
ML00051 / Apr.2020
Chloride SCC of 316 Heat Exchanger Plate
M - Austenitic Stainless SteelP - Heat Exchanger PartAp - FPSOCd - Stress Corrosion
Cm - Micrography by OM using A262 Method ADf - Corrosion Cracking
ML00018 — SCC in Boiler Steam DrumM - Low Carbon SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Ferritic perlitic structure of the shell plate.
207
ML00018 / Apr.2017
SCC in Boiler Steam Drum
M - Low Carbon SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite
Macrography of a transverse section of the steam drum sample that was removed after the inspection had detected multiple cracks propagating into the thickness, more than 50% deep in the thickness.
190
ML00018 / Apr.2017
SCC in Boiler Steam Drum
M - Low Carbon SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - NItal Etched MacroDf - Transverse Section
Micrography of the crack at the internal surface of the steam drum.  The shell plate presents a ferritic perlitic structure.
162
ML00018 / Apr.2017
SCC in Boiler Steam Drum
M - Low Carbon SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Branched Cracks
Micrography of a crack, in a sample as polished, presenting the opened crack.
144
ML00018 / Apr.2017
SCC in Boiler Steam Drum
M - Low Carbon SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Micrography by OMDf - Branched Cracks
Stress corrosion cracks propagating in the ferritic-perlitic structure.
120
ML00018 / Apr.2017
SCC in Boiler Steam Drum
M - Low Carbon SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Branched Cracks

+3 more from this case →

ML00020 — Intergranular SCC in Boiler Steam Drum RepairM - Low Carbon SteelP - Repair WeldAp - BoilerCd - Stress Corrosion
Aspect of the drum shell after removing the tubes and macroetching, indicating that the cracks were located in repair welded regions.
342
ML00020 / Apr.2017
Intergranular SCC in Boiler Steam Drum Repair
M - Low Carbon SteelP - Repair WeldAp - BoilerCd - Stress Corrosion
Cm - Aspect by NDTDf - Cracks
A small sample was removed from the steam drum and the micrography shows that the cracks are intergranular (previous austenite) and located in the weld metal.
285
ML00020 / Apr.2017
Intergranular SCC in Boiler Steam Drum Repair
M - Low Carbon SteelP - Repair WeldAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Corrosion Cracking
The micrography of the small sample removed from the steam drum shows that the cracks are intergranular (previous austenite) and located in the weld metal.
274
ML00020 / Apr.2017
Intergranular SCC in Boiler Steam Drum Repair
M - Low Carbon SteelP - Repair WeldAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Corrosion Cracking
Secondary cracks in the weld metal showing an intergranular morphology. Stress Corrosion Cracking.
249
ML00020 / Apr.2017
Intergranular SCC in Boiler Steam Drum Repair
M - Low Carbon SteelP - Repair WeldAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Corrosion Cracking
Detail of the secondary cracks in the weld metal with intergranular morphology. Stress Corrosion Cracking.
251
ML00020 / Apr.2017
Intergranular SCC in Boiler Steam Drum Repair
M - Low Carbon SteelP - Repair WeldAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Corrosion Cracking

+1 more from this case →

ML00016 — SCC in Free Cutting 303SSM - Austenitic Stainless SteelP - Machined PartAp - OffshoreCd - Stress Corrosion
Regions of the localized corrosion spots associated to non metallic inclusions.
123
ML00016 / Apr.2017
SCC in Free Cutting 303SS
M - Austenitic Stainless SteelP - Machined PartAp - OffshoreCd - Stress Corrosion
Cm - Surface Aspect by SEMDf - Non Metallic Inclusions
The macrography of the longitudinal section of the pin (9.5 mm nominal diameter) shows the localized corrosion associated to the non metallic inclusions.
107
ML00016 / Apr.2017
SCC in Free Cutting 303SS
M - Austenitic Stainless SteelP - Machined PartAp - OffshoreCd - Stress Corrosion
Cm - Macro Oxalic Acid Electrolytic EtchedDf - Localized Corrosion
ML00016 / Apr.2017
SCC in Free Cutting 303SS
M - Austenitic Stainless SteelP - Machined PartAp - OffshoreCd - Stress Corrosion
Cm - Micrography by OM using A262 Method ADf - Localized Corrosion
ML00016 / Apr.2017
SCC in Free Cutting 303SS
M - Austenitic Stainless SteelP - Machined PartAp - OffshoreCd - Stress Corrosion
Cm - Micrography by OM using A262 Method ADf - Non Metallic Inclusions
ML00016 / Apr.2017
SCC in Free Cutting 303SS
M - Austenitic Stainless SteelP - Machined PartAp - OffshoreCd - Stress Corrosion
Cm - Micrography by OM using A262 Method ADf - Localized Corrosion

+3 more from this case →

most recent

The location of the threaded fitting started leaking after less than five years in service. 
Although the corrosion rate was not high, the localized material loss in the threaded surface of the carbon steel flange allowed the connection leakage.
769
ML00184 / Apr.2023
Dissimilar Steels in a Threaded Connection
M - Low Carbon SteelP - ForgingAp - OffshoreCd - Localized Dissolution
Cm - Aspect Before AnalysisDf - General View
Front wheel 17 x 7J of a passenger vehicle (identified as WHEEL 1) that broke during a car accident on a road.
1644
ML00183 / Dec.2022
Ductile Behavior of an Aluminum Wheel
M - Aluminum Silicon MagnesiumP - CastingAp - AutomotiveCd - Ductile Behavior
Cm - Aspect Before AnalysisDf - General View
Tool fixture 5" long, nominal diameter 2", presenting a recess 1/2" deep from two sides.  The rupture occurred about 2" from the end of the rod.   Scale in milimeters.
523
ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Aspect Before AnalysisDf - General View
Pinion of hypoid gearbox, assembled in a 1560-mm long shaft that operated during more than 60,000 hours, and removed from service due to unacceptable wear damage.
1028
ML00181 / Apr.2022
Wear of a Carburized Hypoid Gear
M - Low Alloy for Thermochemical TreatmentP - Pinion-crown assemblyAp - ShipCd - Wear
Cm - Aspect Before AnalysisDf - General View
Aspect of the 3 1/2" diameter tube after the water leakage in high temperature.
962
ML00180 / Mar.2022
Local Melting of Copper Cooling Tubes
M - Pure CopperP - Cooling TubeAp - SiderurgyCd - Overheating
Cm - Aspect Before AnalysisDf - General View
2" drain line from the main 10" line. The leakage occurred at the margin of the weld, a short time after the introduction of the reinforced ribs to reduce vibration.
641
ML00179 / Feb.2022
Hydrides in Titanium Weld
M - Unalloyed TitaniumP - In Field WeldAp - Chemical IndustryCd - Hydride Formation
Cm - Field photoDf - General View
The drilling connector, 21" diameter, presented a crack at the margin of the weld in the forging side (left side of the weld in the figure).
744
ML00178 / Jan.2022
Cold cracks in Cr-Mo Welded Forging
M - CrMo SteelP - ForgingAp - O&G Well DrillingCd - Welding Defect
Cm - Aspect Before AnalysisDf - General View
Macrography of the longitudinally seam weld of the 24" diameter tube, showing that it was welded from both sides and there is a segregation line in the center of the tube thickness.
737
ML00177 / Dec.2021
Cr-Mo Seam Welded Tube
M - CrMo SteelP - Longitudinally Seam WeldedAp - Fired HeaterCd - Not according to spec
Cm - NItal Etched MacroDf - Seam
The titanium rotor blade of a flowmeter broke after two years in service in an acid environment, containing H2S.
339
ML00176 / Nov.2021
Hydride Formation in a Titanium Blade
M - Unalloyed TitaniumP - BladeAp - Oil and GasCd - Hydride Formation
Cm - Aspect Before AnalysisDf - General View
Aspect of the wire rope, 1 1/2" diameter, presenting regions of flattened  areas at the surface of the outer wires. It is a 6 x 19 Seale construction, right regular lay.
552
ML00175 / Aug.2021
Localized External Wear of a Wire Rope
M - High Carbon SteelP - Wire RopeAp - Oil and GasCd - Wear
Cm - Aspect Before AnalysisDf - General View
The carcass was manufactured using niobium stabilized plates, grade AISI 347, with circumferential welds, where the through wall cracks were detected.
300
ML00174 / Jul.2021
Carburization of a 347 SS Welded Joint
M - Austenitic Stainless SteelP - Fabrication WeldAp - EnergyCd - Carburization
Cm - Field photoDf - General View
Aged microstructure of the HP stainless steel, modified with 1%Nb, cast fitting, tubular, operating for 6 years in a furnace which design temperature is 1100°C.  The material presented a network of primary carbides, white and grey, and an austenitic matrix with coalescing secondary precipitation. Some voids. The Vickers identation indicates a hardness value about 260HV 100g in the aged austenitic matrix.
491
ML00173 / May.2021
Welding Cracks in an Aged HP Cast Fitting
M - Heat Resistant SteelP - Cast FtittingAp - PetrochemicalCd - Welding
Cm - Kalling Etched Micrography by OMDf - Microhardness identations
TECMETAL