THE MATERIALS ATLAS.
DISCOVER IT.

About the atlas

Crevice Corrosion in a Subsea System — Aspect Before Analysis

20 images

M

Material

79 classified

Browse all Material →
P

Product

96 classified

Browse all Product →
Ap

Application

37 classified

Browse all Application →
C

Condition

84 classified

Browse all Condition →
Cm

Capture method

52 classified

Browse all Capture method →
Df

Detail focus

208 classified

Browse all Detail focus →

Sharpest next filters

Browse by category (2)
20 images
ML00171 / Feb.2021
Corrosion Fatigue of U Bolt Pipe Clamp
M - Low Carbon SteelP - BoltAp - ShipCd - Corrosion Fatigue
Cm - Fractography by SEMDf - Fracture
ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Fractography by SEMDf - At the Surface
ML00085 / Nov.2017
Corrosion Fatigue of a Martensitic SS Pin
M - Martensitic Stainless SteelP - Forged PinAp - O&G Well DrillingCd - Corrosion Fatigue
Cm - Fractography by SEMDf - Fatigue Striation
ML00094 / Sep.2017
MIC of a Subsea Hydraulic Line
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Behavior
Cm - Fractography by SEMDf - Transgranular Fracture
ML00080 / Sep.2017
MIC of Stacking Disc Springs
M - Low Alloy Medium Carbon QTP - SpringAp - SubseaCd - Brittle Behavior
Cm - Fractography by SEMDf - Intergranular Fracture
The fracture surface, although presenting a large amount of corrosion products, shows also evidences of a brittle behavior with regions of cleavage micromechanism.
116
ML00002 / Jan.2018
Preferential Dissolution and Cracks in SDSS
M - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Cm - Fractography by SEMDf - Cleavage Facets

More from these cases

ML00137 — Brittle Fracture of a 15-5 PH Valve SpringM - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Fractography by SEMDf - Intergranular Fracture
ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Fractography by SEMDf - Intergranular Fracture
ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Fractography by SEMDf - Fracture
ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Fractography by SEMDf - Fracture
ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Fractography by SEMDf - Transgranular Fracture

+2 more from this case →

ML00085 — Corrosion Fatigue of a Martensitic SS PinM - Martensitic Stainless SteelP - Forged PinAp - O&G Well DrillingCd - Corrosion Fatigue
ML00085 / Nov.2017
Corrosion Fatigue of a Martensitic SS Pin
M - Martensitic Stainless SteelP - Forged PinAp - O&G Well DrillingCd - Corrosion Fatigue
Cm - Fractography by SEMDf - Dimples
ML00080 — MIC of Stacking Disc SpringsM - Low Alloy Medium Carbon QTP - SpringAp - SubseaCd - Brittle Behavior
ML00080 / Sep.2017
MIC of Stacking Disc Springs
M - Low Alloy Medium Carbon QTP - SpringAp - SubseaCd - Brittle Behavior
Cm - Fractography by SEMDf - Intergranular Fracture
ML00080 / Sep.2017
MIC of Stacking Disc Springs
M - Low Alloy Medium Carbon QTP - SpringAp - SubseaCd - Brittle Behavior
Cm - Fractography by SEMDf - Intergranular Fracture
ML00080 / Sep.2017
MIC of Stacking Disc Springs
M - Low Alloy Medium Carbon QTP - SpringAp - SubseaCd - Brittle Behavior
Cm - Fractography by SEMDf - Transgranular Fracture
ML00080 / Sep.2017
MIC of Stacking Disc Springs
M - Low Alloy Medium Carbon QTP - SpringAp - SubseaCd - Brittle Behavior
Cm - Fractography by SEMDf - Transgranular Fracture
ML00002 — Preferential Dissolution and Cracks in SDSSM - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
ML00002 / Jan.2018
Preferential Dissolution and Cracks in SDSS
M - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Cm - Fractography by SEMDf - Cleavage Facets
ML00002 / Jan.2018
Preferential Dissolution and Cracks in SDSS
M - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Cm - Fractography by SEMDf - Cleavage Facets

most recent

The location of the threaded fitting started leaking after less than five years in service. 
Although the corrosion rate was not high, the localized material loss in the threaded surface of the carbon steel flange allowed the connection leakage.
770
ML00184 / Apr.2023
Dissimilar Steels in a Threaded Connection
M - Low Carbon SteelP - ForgingAp - OffshoreCd - Localized Dissolution
Cm - Aspect Before AnalysisDf - General View
Front wheel 17 x 7J of a passenger vehicle (identified as WHEEL 1) that broke during a car accident on a road.
1645
ML00183 / Dec.2022
Ductile Behavior of an Aluminum Wheel
M - Aluminum Silicon MagnesiumP - CastingAp - AutomotiveCd - Ductile Behavior
Cm - Aspect Before AnalysisDf - General View
Tool fixture 5" long, nominal diameter 2", presenting a recess 1/2" deep from two sides.  The rupture occurred about 2" from the end of the rod.   Scale in milimeters.
523
ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Aspect Before AnalysisDf - General View
Pinion of hypoid gearbox, assembled in a 1560-mm long shaft that operated during more than 60,000 hours, and removed from service due to unacceptable wear damage.
1028
ML00181 / Apr.2022
Wear of a Carburized Hypoid Gear
M - Low Alloy for Thermochemical TreatmentP - Pinion-crown assemblyAp - ShipCd - Wear
Cm - Aspect Before AnalysisDf - General View
Aspect of the 3 1/2" diameter tube after the water leakage in high temperature.
963
ML00180 / Mar.2022
Local Melting of Copper Cooling Tubes
M - Pure CopperP - Cooling TubeAp - SiderurgyCd - Overheating
Cm - Aspect Before AnalysisDf - General View
2" drain line from the main 10" line. The leakage occurred at the margin of the weld, a short time after the introduction of the reinforced ribs to reduce vibration.
642
ML00179 / Feb.2022
Hydrides in Titanium Weld
M - Unalloyed TitaniumP - In Field WeldAp - Chemical IndustryCd - Hydride Formation
Cm - Field photoDf - General View
The drilling connector, 21" diameter, presented a crack at the margin of the weld in the forging side (left side of the weld in the figure).
748
ML00178 / Jan.2022
Cold cracks in Cr-Mo Welded Forging
M - CrMo SteelP - ForgingAp - O&G Well DrillingCd - Welding Defect
Cm - Aspect Before AnalysisDf - General View
Macrography of the longitudinally seam weld of the 24" diameter tube, showing that it was welded from both sides and there is a segregation line in the center of the tube thickness.
737
ML00177 / Dec.2021
Cr-Mo Seam Welded Tube
M - CrMo SteelP - Longitudinally Seam WeldedAp - Fired HeaterCd - Not according to spec
Cm - NItal Etched MacroDf - Seam
The titanium rotor blade of a flowmeter broke after two years in service in an acid environment, containing H2S.
340
ML00176 / Nov.2021
Hydride Formation in a Titanium Blade
M - Unalloyed TitaniumP - BladeAp - Oil and GasCd - Hydride Formation
Cm - Aspect Before AnalysisDf - General View
Aspect of the wire rope, 1 1/2" diameter, presenting regions of flattened  areas at the surface of the outer wires. It is a 6 x 19 Seale construction, right regular lay.
553
ML00175 / Aug.2021
Localized External Wear of a Wire Rope
M - High Carbon SteelP - Wire RopeAp - Oil and GasCd - Wear
Cm - Aspect Before AnalysisDf - General View
The carcass was manufactured using niobium stabilized plates, grade AISI 347, with circumferential welds, where the through wall cracks were detected.
303
ML00174 / Jul.2021
Carburization of a 347 SS Welded Joint
M - Austenitic Stainless SteelP - Fabrication WeldAp - EnergyCd - Carburization
Cm - Field photoDf - General View
Aged microstructure of the HP stainless steel, modified with 1%Nb, cast fitting, tubular, operating for 6 years in a furnace which design temperature is 1100°C.  The material presented a network of primary carbides, white and grey, and an austenitic matrix with coalescing secondary precipitation. Some voids. The Vickers identation indicates a hardness value about 260HV 100g in the aged austenitic matrix.
493
ML00173 / May.2021
Welding Cracks in an Aged HP Cast Fitting
M - Heat Resistant SteelP - Cast FtittingAp - PetrochemicalCd - Welding
Cm - Kalling Etched Micrography by OMDf - Microhardness identations