THE MATERIALS ATLAS.
DISCOVER IT.

About the atlas

Crevice Corrosion in a Subsea System — Aspect Before Analysis

19 images

M

Material

79 classified

Browse all Material →
P

Product

96 classified

Browse all Product →
Ap

Application

37 classified

Browse all Application →
C

Condition

84 classified

Browse all Condition →
Cm

Capture method

52 classified

Browse all Capture method →
Df

Detail focus

208 classified

Browse all Detail focus →

Sharpest next filters

Browse by category (1)
19 images
The macrography of a longitudinal section of the shell plate (sample removed from the boiler), at the position of the fillet weld (sealing weld) with a tube, where surface welding repairs created conditions for cracking the base material in a transgranular morphology. Several cracks were identify starting from the steam drum internal surface.
448
ML00019 / Apr.2017
Transgranular SCC in Boiler Steam Drum
M - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Transverse Section AspectDf - Cracks
Typical branched stress corrosion cracks in a low carbon steel, ferritic-pertlitic structure. The cracks are filled with corrosion products.
771
ML00018 / Apr.2017
SCC in Boiler Steam Drum
M - Low Carbon SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Branched Cracks

More from these cases

ML00019 — Transgranular SCC in Boiler Steam DrumM - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Schematic drawing presenting the longitudinal section of the shell plate (sample removed from the boiler), at the position of the fillet weld (sealing weld) with a tube,  where surface welding repairs created conditions for cracking the base material in a transgranular morphology. Several cracks were identify starting from the steam drum internal surface.
120
ML00019 / Apr.2017
Transgranular SCC in Boiler Steam Drum
M - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Identification drawingDf - Cracks
Micrography of a transverse section of the shell plate in a cracked position showing the transgranular morphology of the stress corrosion cracks.
167
ML00019 / Apr.2017
Transgranular SCC in Boiler Steam Drum
M - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by SEMDf - Transgranular Cracking
ML00019 / Apr.2017
Transgranular SCC in Boiler Steam Drum
M - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite
ML00019 / Apr.2017
Transgranular SCC in Boiler Steam Drum
M - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite
ML00019 / Apr.2017
Transgranular SCC in Boiler Steam Drum
M - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Branched Cracks

+4 more from this case →

ML00018 — SCC in Boiler Steam DrumM - Low Carbon SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Ferritic perlitic structure of the shell plate.
207
ML00018 / Apr.2017
SCC in Boiler Steam Drum
M - Low Carbon SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite
Macrography of a transverse section of the steam drum sample that was removed after the inspection had detected multiple cracks propagating into the thickness, more than 50% deep in the thickness.
190
ML00018 / Apr.2017
SCC in Boiler Steam Drum
M - Low Carbon SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - NItal Etched MacroDf - Transverse Section
Micrography of the crack at the internal surface of the steam drum.  The shell plate presents a ferritic perlitic structure.
162
ML00018 / Apr.2017
SCC in Boiler Steam Drum
M - Low Carbon SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Branched Cracks
Micrography of a crack, in a sample as polished, presenting the opened crack.
144
ML00018 / Apr.2017
SCC in Boiler Steam Drum
M - Low Carbon SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Micrography by OMDf - Branched Cracks
Stress corrosion cracks propagating in the ferritic-perlitic structure.
120
ML00018 / Apr.2017
SCC in Boiler Steam Drum
M - Low Carbon SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Branched Cracks

+3 more from this case →

most recent

The location of the threaded fitting started leaking after less than five years in service. 
Although the corrosion rate was not high, the localized material loss in the threaded surface of the carbon steel flange allowed the connection leakage.
770
ML00184 / Apr.2023
Dissimilar Steels in a Threaded Connection
M - Low Carbon SteelP - ForgingAp - OffshoreCd - Localized Dissolution
Cm - Aspect Before AnalysisDf - General View
Front wheel 17 x 7J of a passenger vehicle (identified as WHEEL 1) that broke during a car accident on a road.
1645
ML00183 / Dec.2022
Ductile Behavior of an Aluminum Wheel
M - Aluminum Silicon MagnesiumP - CastingAp - AutomotiveCd - Ductile Behavior
Cm - Aspect Before AnalysisDf - General View
Tool fixture 5" long, nominal diameter 2", presenting a recess 1/2" deep from two sides.  The rupture occurred about 2" from the end of the rod.   Scale in milimeters.
523
ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Aspect Before AnalysisDf - General View
Pinion of hypoid gearbox, assembled in a 1560-mm long shaft that operated during more than 60,000 hours, and removed from service due to unacceptable wear damage.
1028
ML00181 / Apr.2022
Wear of a Carburized Hypoid Gear
M - Low Alloy for Thermochemical TreatmentP - Pinion-crown assemblyAp - ShipCd - Wear
Cm - Aspect Before AnalysisDf - General View
Aspect of the 3 1/2" diameter tube after the water leakage in high temperature.
963
ML00180 / Mar.2022
Local Melting of Copper Cooling Tubes
M - Pure CopperP - Cooling TubeAp - SiderurgyCd - Overheating
Cm - Aspect Before AnalysisDf - General View
2" drain line from the main 10" line. The leakage occurred at the margin of the weld, a short time after the introduction of the reinforced ribs to reduce vibration.
642
ML00179 / Feb.2022
Hydrides in Titanium Weld
M - Unalloyed TitaniumP - In Field WeldAp - Chemical IndustryCd - Hydride Formation
Cm - Field photoDf - General View
The drilling connector, 21" diameter, presented a crack at the margin of the weld in the forging side (left side of the weld in the figure).
748
ML00178 / Jan.2022
Cold cracks in Cr-Mo Welded Forging
M - CrMo SteelP - ForgingAp - O&G Well DrillingCd - Welding Defect
Cm - Aspect Before AnalysisDf - General View
Macrography of the longitudinally seam weld of the 24" diameter tube, showing that it was welded from both sides and there is a segregation line in the center of the tube thickness.
737
ML00177 / Dec.2021
Cr-Mo Seam Welded Tube
M - CrMo SteelP - Longitudinally Seam WeldedAp - Fired HeaterCd - Not according to spec
Cm - NItal Etched MacroDf - Seam
The titanium rotor blade of a flowmeter broke after two years in service in an acid environment, containing H2S.
340
ML00176 / Nov.2021
Hydride Formation in a Titanium Blade
M - Unalloyed TitaniumP - BladeAp - Oil and GasCd - Hydride Formation
Cm - Aspect Before AnalysisDf - General View
Aspect of the wire rope, 1 1/2" diameter, presenting regions of flattened  areas at the surface of the outer wires. It is a 6 x 19 Seale construction, right regular lay.
553
ML00175 / Aug.2021
Localized External Wear of a Wire Rope
M - High Carbon SteelP - Wire RopeAp - Oil and GasCd - Wear
Cm - Aspect Before AnalysisDf - General View
The carcass was manufactured using niobium stabilized plates, grade AISI 347, with circumferential welds, where the through wall cracks were detected.
303
ML00174 / Jul.2021
Carburization of a 347 SS Welded Joint
M - Austenitic Stainless SteelP - Fabrication WeldAp - EnergyCd - Carburization
Cm - Field photoDf - General View
Aged microstructure of the HP stainless steel, modified with 1%Nb, cast fitting, tubular, operating for 6 years in a furnace which design temperature is 1100°C.  The material presented a network of primary carbides, white and grey, and an austenitic matrix with coalescing secondary precipitation. Some voids. The Vickers identation indicates a hardness value about 260HV 100g in the aged austenitic matrix.
493
ML00173 / May.2021
Welding Cracks in an Aged HP Cast Fitting
M - Heat Resistant SteelP - Cast FtittingAp - PetrochemicalCd - Welding
Cm - Kalling Etched Micrography by OMDf - Microhardness identations
TECMETAL