Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00124 / Feb.2018
MIC of a Martensitic Valve Ring
M - Martensitic Stainless SteelP - ForgingAp - EnergyCd - Brittle Behavior
Cm - Kalling Etched Micrography by OMDf - Martensite
ML00123 / Feb.2018
Non Qualified Superduplex for Subsea
M - Super Duplex Stainless SteelP - BarAp - Oil and GasCd - Not according to spec
Cm - NaOH Electrolytic Etched MicroDf - Ferrite and Austenite
Micrography of the case, observed in the center of the thickness, showing an equiaxial granular austenitic microstructure, free from carbides.  The structure is typical of a 316 SS, in a solution annealed condition.
176
ML00122 / Feb.2018
Crevice Corrosion in a Subsea System
M - Austenitic Stainless SteelP - CaseAp - Oil and GasCd - Crevice
Cm - Micrography by OM using A262 Method ADf - Austenite
Nitronic 60 cylinder. Micrography of the longitudinal section in the center of the thickness, presenting a fully austenitic microstructure, equiaxial grains, and evidences of the manufacturing process by hot forming.
179
ML00121 / Feb.2018
Pitting Corrosion in a Subsea System
M - Austenitic / MartensiticP - Rod & CylinderAp - SubseaCd - Pitting Corrosion
Cm - Micrography by OM using A262 Method ADf - Austenite
Micrography of a longitudinal section of the bolt in the center of the thickness, presenting a ferritic pearlitic structure with elongated grains due to the forming process, without later heat treatment.
173
ML00120 / Jun.2018
Ductile Rupture of a Carbon Steel Eye Bolt
M - Low Carbon SteelP - FastenerAp - AutomotiveCd - Overload
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite
Micrography of the plate in a longitudinal section, presenting a typical ferritic pearlitic structure, banded.  The plate is 22 mm thick.
182
ML00119 / Feb.2018
Thermal Fatigue of a Marine Boiler
M - Low Carbon SteelP - Fabrication WeldAp - ShipCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Banded Structure
ML00110 / Jan.2018
Non Conformance in Spray and Fuse Pin
M - Low Alloy Medium Carbon QTP - Tubular ForgingAp - O&G Well DrillingCd - Heat Treatment Defect
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite
Micrography of a transverse section of the pipe, external diameter 33.4 mm schedule XXS, in the center of the 9.1 mm thickness.  The structure is predominantly ferritic.  Small amount of pearlite.
556
ML00112 / Dec.2017
1" XXS Pipe Not Qualified For Low Temp
M - Low Carbon SteelP - Seamless PipeAp - RefineryCd - Not according to spec
Cm - Nital Etched Micrography by OMDf - Predominantly Ferritic

More from these cases

ML00124 — MIC of a Martensitic Valve RingM - Martensitic Stainless SteelP - ForgingAp - EnergyCd - Brittle Behavior
ML00124 / Feb.2018
MIC of a Martensitic Valve Ring
M - Martensitic Stainless SteelP - ForgingAp - EnergyCd - Brittle Behavior
Cm - Kalling Etched Micrography by OMDf - Martensite
ML00123 — Non Qualified Superduplex for SubseaM - Super Duplex Stainless SteelP - BarAp - Oil and GasCd - Not according to spec
ML00123 / Feb.2018
Non Qualified Superduplex for Subsea
M - Super Duplex Stainless SteelP - BarAp - Oil and GasCd - Not according to spec
Cm - NaOH Electrolytic Etched MicroDf - Ferrite and Austenite
ML00122 — Crevice Corrosion in a Subsea SystemM - Austenitic Stainless SteelP - CaseAp - Oil and GasCd - Crevice
Micrographic detail of the fully austenitic granular structure of the case, in the center of the thickness.
158
ML00122 / Feb.2018
Crevice Corrosion in a Subsea System
M - Austenitic Stainless SteelP - CaseAp - Oil and GasCd - Crevice
Cm - Micrography by OM using A262 Method ADf - Austenite
ML00121 — Pitting Corrosion in a Subsea SystemM - Austenitic / MartensiticP - Rod & CylinderAp - SubseaCd - Pitting Corrosion
Nitronic 60 cylinder. Micrography of the longitudinal section in the center of the thickness, presenting a fully austenitic microstructure, with some aligned non metallic inclusions.
157
ML00121 / Feb.2018
Pitting Corrosion in a Subsea System
M - Austenitic / MartensiticP - Rod & CylinderAp - SubseaCd - Pitting Corrosion
Cm - Micrography by OM using A262 Method ADf - Austenite
Nitronic 60 cylinder. Micrographic detail of the longitudinal section in the center of the thickness, presenting a fully austenitic microstructure, equiaxial grains, typical of a solution annealed condition.
136
ML00121 / Feb.2018
Pitting Corrosion in a Subsea System
M - Austenitic / MartensiticP - Rod & CylinderAp - SubseaCd - Pitting Corrosion
Cm - Micrography by OM using A262 Method ADf - Austenite
Nitronic 60 cylinder. Micrography of the longitudinal section close to the surface, presenting a fully austenitic microstructure, with a shadow close to the external surface that is associated to a small layer of strain hardened structure (deformation twins).
133
ML00121 / Feb.2018
Pitting Corrosion in a Subsea System
M - Austenitic / MartensiticP - Rod & CylinderAp - SubseaCd - Pitting Corrosion
Cm - Micrography by OM using A262 Method ADf - Strain Hardened
Nitronic 60 cylinder. Micrography of the longitudinal section close to the surface, presenting a fully austenitic microstructure, with a 0.15mm layer of strain hardened structure (deformation twins).
120
ML00121 / Feb.2018
Pitting Corrosion in a Subsea System
M - Austenitic / MartensiticP - Rod & CylinderAp - SubseaCd - Pitting Corrosion
Cm - Micrography by OM using A262 Method ADf - Strain Hardened
Nitronic 60 cylinder. Micrographic detail of the longitudinal section close to the surface, presenting a fully austenitic microstructure, with a layer of strain hardened structure (deformation twins).
113
ML00121 / Feb.2018
Pitting Corrosion in a Subsea System
M - Austenitic / MartensiticP - Rod & CylinderAp - SubseaCd - Pitting Corrosion
Cm - Micrography by OM using A262 Method ADf - Strain Hardened

+3 more from this case →

ML00120 — Ductile Rupture of a Carbon Steel Eye BoltM - Low Carbon SteelP - FastenerAp - AutomotiveCd - Overload
Micrographic detail of the ferritic pearlitic structure, with grains sligthly elongated.
157
ML00120 / Jun.2018
Ductile Rupture of a Carbon Steel Eye Bolt
M - Low Carbon SteelP - FastenerAp - AutomotiveCd - Overload
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite
Micrographic detail of a longitudinal section of the bolt at the bottom of the thread fillet, presenting a plastically deformed ferritic pearlitic structure.  This analysis was conducted far from the failure and the structure was created by the cold forming process to manufacture the thread.
147
ML00120 / Jun.2018
Ductile Rupture of a Carbon Steel Eye Bolt
M - Low Carbon SteelP - FastenerAp - AutomotiveCd - Overload
Cm - Nital Etched Micrography by OMDf - Strain Hardened
ML00119 — Thermal Fatigue of a Marine BoilerM - Low Carbon SteelP - Fabrication WeldAp - ShipCd - Thermal Fatigue
Micrography of the plate in a longitudinal section, presenting a typical ferritic pearlitic structure, banded.
165
ML00119 / Feb.2018
Thermal Fatigue of a Marine Boiler
M - Low Carbon SteelP - Fabrication WeldAp - ShipCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite
Micrographic detail of the ferritic pearlitic structure of the plate in the longitudinal section.
147
ML00119 / Feb.2018
Thermal Fatigue of a Marine Boiler
M - Low Carbon SteelP - Fabrication WeldAp - ShipCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite
Micrography of the weld metal in the center os the weld. Columnar grains (of the previous austenite) with primary ferrite in the grain boundaries and acicular ferrite intragranular.
125
ML00119 / Feb.2018
Thermal Fatigue of a Marine Boiler
M - Low Carbon SteelP - Fabrication WeldAp - ShipCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Ferritic Weld Metal
Micrographic detail of the weld metal in the center os the weld. Columnar grains (of the previous austenite) with primary ferrite in the grain boundaries; and details of the ferrite with aligned second phases and acicular ferrite, intragranular.
112
ML00119 / Feb.2018
Thermal Fatigue of a Marine Boiler
M - Low Carbon SteelP - Fabrication WeldAp - ShipCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Ferritic Weld Metal
Micrography of the tube HAZ in a region of (austenitic) grain coarse, presenting a bainitic structure.
105
ML00119 / Feb.2018
Thermal Fatigue of a Marine Boiler
M - Low Carbon SteelP - Fabrication WeldAp - ShipCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Bainitic HAZ

+6 more from this case →

ML00110 — Non Conformance in Spray and Fuse PinM - Low Alloy Medium Carbon QTP - Tubular ForgingAp - O&G Well DrillingCd - Heat Treatment Defect
ML00110 / Jan.2018
Non Conformance in Spray and Fuse Pin
M - Low Alloy Medium Carbon QTP - Tubular ForgingAp - O&G Well DrillingCd - Heat Treatment Defect
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite
ML00110 / Jan.2018
Non Conformance in Spray and Fuse Pin
M - Low Alloy Medium Carbon QTP - Tubular ForgingAp - O&G Well DrillingCd - Heat Treatment Defect
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite
ML00112 — 1" XXS Pipe Not Qualified For Low TempM - Low Carbon SteelP - Seamless PipeAp - RefineryCd - Not according to spec
ML00112 / Dec.2017
1" XXS Pipe Not Qualified For Low Temp
M - Low Carbon SteelP - Seamless PipeAp - RefineryCd - Not according to spec
Cm - Nital Etched Micrography by OMDf - Predominantly Ferritic
ML00112 / Dec.2017
1" XXS Pipe Not Qualified For Low Temp
M - Low Carbon SteelP - Seamless PipeAp - RefineryCd - Not according to spec
Cm - Nital Etched Micrography by OMDf - Predominantly Ferritic