Tube

2 cases · 5 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00052 / Apr.2017
Cold Cracks in API 5CT L80 Tube Welded to a Structural Part
M - Low Alloy SteelP - Seamless tubeAp - OffshoreCd - Welding Defect
Cm - Nital Etched Micrography by OMDf - Fusion Line
ML00026 / Feb.2017
Autogenous Seam Welded Tube in Ferritic SS
M - Ferritic Stainless SteelP - Fabrication WeldAp - AutomotiveCd - Typical manufacturing
Cm - Kalling Etched Micrography by OMDf - Fusion Line

More from these cases

ML00052 — Cold Cracks in API 5CT L80 Tube Welded to a Structural PartM - Low Alloy SteelP - Seamless tubeAp - OffshoreCd - Welding Defect
ML00052 / Apr.2017
Cold Cracks in API 5CT L80 Tube Welded to a Structural Part
M - Low Alloy SteelP - Seamless tubeAp - OffshoreCd - Welding Defect
Cm - Nital Etched Micrography by SEMDf - Fusion Line
ML00052 / Apr.2017
Cold Cracks in API 5CT L80 Tube Welded to a Structural Part
M - Low Alloy SteelP - Seamless tubeAp - OffshoreCd - Welding Defect
Cm - Nital Etched Micrography by SEMDf - Fusion Line
ML00026 — Autogenous Seam Welded Tube in Ferritic SSM - Ferritic Stainless SteelP - Fabrication WeldAp - AutomotiveCd - Typical manufacturing
ML00026 / Feb.2017
Autogenous Seam Welded Tube in Ferritic SS
M - Ferritic Stainless SteelP - Fabrication WeldAp - AutomotiveCd - Typical manufacturing
Cm - Kalling Etched Micrography by OMDf - Fusion Line