A
3 cases · 5 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis
Condition: Damage ×Capture method: Optical Microscope ×Detail focus: Intragranular Secondary Precipitation ×clear all
A — sub-branches

ML00086 / Nov.2017
Intergranular Corrosion of Sensitized 304SS
M - Austenitic Stainless SteelP - Seamless tubeAp - Heat ExchangerCd - Intergranular Corrosion
Cm - Micrography by OM using A262 Method ADf - Intragranular Secondary Precipitation

ML00097 / Nov.2017
Cast SS Tube Removed From High Temperature Service
M - Heat Resistant SteelP - Centrifugally Cast PipeAp - SiderurgyCd - High Temperature
Cm - Glyceregia Etched Micrography by OMDf - Intragranular Secondary Precipitation

ML00038 / Apr.2017
Cast SS Tube for High Temperature Service
M - Heat Resistant SteelP - Centrifugally Cast PipeAp - SiderurgyCd - Creep
Cm - Glyceregia Etched Micrography by OMDf - Intragranular Secondary Precipitation
More from these cases

ML00086 / Nov.2017
Intergranular Corrosion of Sensitized 304SS
M - Austenitic Stainless SteelP - Seamless tubeAp - Heat ExchangerCd - Intergranular Corrosion
Cm - Micrography by OM using A262 Method ADf - Intragranular Secondary Precipitation

ML00086 / Nov.2017
Intergranular Corrosion of Sensitized 304SS
M - Austenitic Stainless SteelP - Seamless tubeAp - Heat ExchangerCd - Intergranular Corrosion
Cm - Micrography by OM using A262 Method ADf - Intragranular Secondary Precipitation