Sulfide Inclusions

1 case · 3 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00035 / Dec.2017
Carbon Steel L Shape
M - Low Carbon SteelP - Rolled ShapeAp - StructureCd - Removed From Service
Cm - Nital Etched Micrography by OMDf - In the Center of the Thickness

More from these cases

ML00035 — Carbon Steel L ShapeM - Low Carbon SteelP - Rolled ShapeAp - StructureCd - Removed From Service
ML00035 / Dec.2017
Carbon Steel L Shape
M - Low Carbon SteelP - Rolled ShapeAp - StructureCd - Removed From Service
Cm - Nital Etched Micrography by OMDf - At the Surface
ML00035 / Dec.2017
Carbon Steel L Shape
M - Low Carbon SteelP - Rolled ShapeAp - StructureCd - Removed From Service
Cm - Nital Etched Micrography by OMDf - Transverse Section