Ferritic pearlitic matrix

3 cases · 31 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Micrography of a crankshaft longitudinal section at the shaft edge, in the as polished condition, presenting nodular graphite, well distruibuted.
139
ML00154 / Jan.2019
High Strength Cast Iron Crankshaft
M - Nodular Cast IronP - CastingAp - EngineCd - Surface treatment
Cm - As polished micrographyDf - At the Surface
Micrography of CAP A, showing graphite in imperfect nodules and ferritic matrix.
481
ML00047 / Mar.2017
Ductile Cast Iron Caps of Electrical Insulators
M - Ductile Cast IronP - Cast iron capAp - EnergyCd - Typical manufacturing
Cm - Nital Etched Micrography by OMDf - Graphite in Imperfect Nodules
Polished cross-section showing rounded graphite nodules within a ferritic matrix, bordered by an irregular oxidized region at the surface edge.
910
ML00001 / Dec.2017
Thermal Fatigue of Cast Iron
M - Nodular Cast IronP - CastAp - SiderurgyCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Oxide Layer

More from these cases

ML00154 — High Strength Cast Iron CrankshaftM - Nodular Cast IronP - CastingAp - EngineCd - Surface treatment
As polished micrography of the crankshaft at the shaft edge, close to the surface.  Graphite in nodules.
126
ML00154 / Jan.2019
High Strength Cast Iron Crankshaft
M - Nodular Cast IronP - CastingAp - EngineCd - Surface treatment
Cm - As polished micrographyDf - Graphite in Nodules
As polished micrographic detail of the graphite in nodules, close to the surface of the shaft edge, in a longitudinal section.
114
ML00154 / Jan.2019
High Strength Cast Iron Crankshaft
M - Nodular Cast IronP - CastingAp - EngineCd - Surface treatment
Cm - As polished micrographyDf - Graphite in Nodules
ML00154 / Jan.2019
High Strength Cast Iron Crankshaft
M - Nodular Cast IronP - CastingAp - EngineCd - Surface treatment
Cm - Nital Etched Micrography by OMDf - At the Surface
ML00154 / Jan.2019
High Strength Cast Iron Crankshaft
M - Nodular Cast IronP - CastingAp - EngineCd - Surface treatment
Cm - Nital Etched Micrography by OMDf - Matrix of ferrite and pearlite
ML00154 / Jan.2019
High Strength Cast Iron Crankshaft
M - Nodular Cast IronP - CastingAp - EngineCd - Surface treatment
Cm - Nital Etched Micrography by OMDf - Matrix of ferrite and pearlite

+12 more from this case →

ML00047 — Ductile Cast Iron Caps of Electrical InsulatorsM - Ductile Cast IronP - Cast iron capAp - EnergyCd - Typical manufacturing
ML00047 / Mar.2017
Ductile Cast Iron Caps of Electrical Insulators
M - Ductile Cast IronP - Cast iron capAp - EnergyCd - Typical manufacturing
Cm - Nital Etched Micrography by OMDf - Predominantly Ferritic
ML00047 / Mar.2017
Ductile Cast Iron Caps of Electrical Insulators
M - Ductile Cast IronP - Cast iron capAp - EnergyCd - Typical manufacturing
Cm - Nital Etched Micrography by OMDf - Graphite in Nodules
ML00047 / Mar.2017
Ductile Cast Iron Caps of Electrical Insulators
M - Ductile Cast IronP - Cast iron capAp - EnergyCd - Typical manufacturing
Cm - Nital Etched Micrography by OMDf - Predominantly Ferritic
ML00047 / Mar.2017
Ductile Cast Iron Caps of Electrical Insulators
M - Ductile Cast IronP - Cast iron capAp - EnergyCd - Typical manufacturing
Cm - Nital Etched Micrography by OMDf - Graphite in Nodules
ML00047 / Mar.2017
Ductile Cast Iron Caps of Electrical Insulators
M - Ductile Cast IronP - Cast iron capAp - EnergyCd - Typical manufacturing
Cm - Nital Etched Micrography by OMDf - Predominantly Ferritic
ML00001 — Thermal Fatigue of Cast IronM - Nodular Cast IronP - CastAp - SiderurgyCd - Thermal Fatigue
The 1" flat casting product presents a ferritic perlitic matrix and graphite nodules.
112
ML00001 / Dec.2017
Thermal Fatigue of Cast Iron
M - Nodular Cast IronP - CastAp - SiderurgyCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Graphite in Nodules
Center of the flat casting product, presenting nodular graphite and ferritic perlitic matrix.
113
ML00001 / Dec.2017
Thermal Fatigue of Cast Iron
M - Nodular Cast IronP - CastAp - SiderurgyCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Predominantly Ferritic Matrix
Nodular cast iron presenting a ferritic perlitic matrix.
109
ML00001 / Dec.2017
Thermal Fatigue of Cast Iron
M - Nodular Cast IronP - CastAp - SiderurgyCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Matrix of ferrite and pearlite
Nodular cast iron.  Ferritic perlitic matrix. White regions in the pearlite colonies are free carbides.
129
ML00001 / Dec.2017
Thermal Fatigue of Cast Iron
M - Nodular Cast IronP - CastAp - SiderurgyCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Free Carbides in Pearlite Colonies
The graphite nodules remain at the surface and the matrix was consumed during high temperature exposition.
117
ML00001 / Dec.2017
Thermal Fatigue of Cast Iron
M - Nodular Cast IronP - CastAp - SiderurgyCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Oxide Layer

+1 more from this case →