Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00076 / Jun.2017
Hydrogen Cracking of a 17-7 PH Subsea Spring
M - Precipitation Hardened Stainless SteelP - WireAp - SubseaCd - Hydrogen Embrittlement
Cm - Kalling Etched Micrography by OMDf - Longitudinal Section
ML00036 / Jan.2018
High Strength Medium Carbon Steel Wire
M - Medium Carbon SteelP - WireAp - OffshoreCd - Typical manufacturing
Cm - Nital Etched Micrography by OMDf - Longitudinal Section

More from these cases

ML00076 — Hydrogen Cracking of a 17-7 PH Subsea SpringM - Precipitation Hardened Stainless SteelP - WireAp - SubseaCd - Hydrogen Embrittlement
ML00076 / Jun.2017
Hydrogen Cracking of a 17-7 PH Subsea Spring
M - Precipitation Hardened Stainless SteelP - WireAp - SubseaCd - Hydrogen Embrittlement
Cm - Kalling Etched Micrography by OMDf - Longitudinal Section
ML00036 — High Strength Medium Carbon Steel WireM - Medium Carbon SteelP - WireAp - OffshoreCd - Typical manufacturing
ML00036 / Jan.2018
High Strength Medium Carbon Steel Wire
M - Medium Carbon SteelP - WireAp - OffshoreCd - Typical manufacturing
Cm - Nital Etched Micrography by OMDf - Longitudinal Section