Internal Surface

3 cases · 3 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00131 / Apr.2018
Brittle Failure of a Soft Roller Bearing
M - Wear Resistant SteelP - Roller BearingAp - Mechanical IndustryCd - Heat Treatment Defect
Cm - Aspect Before AnalysisDf - Internal Surface
ML00092 / Sep.2017
MIC of a Valve Body
M - Martensitic Stainless SteelP - Valve BodyAp - Oil and GasCd - Brittle Behavior
Cm - Aspect Before AnalysisDf - Internal Surface
ML00012 / Aug.2017
Vibration Induced Fatigue in a 316/316L SS
M - Austenitic Stainless SteelP - Seamless PipeAp - OffshoreCd - Vibration Induced Fatigue
Cm - Aspect Before AnalysisDf - Internal Surface