Internal Surface

2 cases · 3 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Aspect of the internal tube surface after a longitudinal cut, without cleaning.  It is possible to see a clean surface inside the tube.
104
ML00165 / Jul.2020
SCC of Aluminum Bronze Heating Coil
M - Aluminum BronzeP - Seamless tubeAp - Oil and GasCd - Stress Corrosion
Cm - Surface AspectDf - Internal Surface
ML00092 / Sep.2017
MIC of a Valve Body
M - Martensitic Stainless SteelP - Valve BodyAp - Oil and GasCd - Brittle Behavior
Cm - Aspect Before AnalysisDf - Internal Surface

More from these cases

ML00165 — SCC of Aluminum Bronze Heating CoilM - Aluminum BronzeP - Seamless tubeAp - Oil and GasCd - Stress Corrosion
ML00165 / Jul.2020
SCC of Aluminum Bronze Heating Coil
M - Aluminum BronzeP - Seamless tubeAp - Oil and GasCd - Stress Corrosion
Cm - Aspect Before AnalysisDf - Internal Surface