Crevice Corrosion in a Subsea System — Aspect Before Analysis

Fracture position at the pipe body, about 1 meter from the tool joint end.  The fracture presented two main aspects, a flat fracture transverse to the pipe axis, that propagated by fatigue through almost 50% of the pipe perimeter, and a final fracture by shear overloading.
560
ML00169 / Nov.2020
Drill Pipe Fracture in the Pipe Body
M - Low Alloy Medium Carbon QTP - Drill PipeAp - O&G Well DrillingCd - Corrosion Fatigue
Cm - Aspect Before AnalysisDf - General View