Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00175 / Aug.2021
Localized External Wear of a Wire Rope
M - High Carbon SteelP - Wire RopeAp - Oil and GasCd - Wear
Cm - Nital Etched Micrography by OMDf - At the Surface

ML00117 / Jan.2018
High Carbon Steel Wire Rope
M - High Carbon SteelP - Wire RopeAp - Oil and GasCd - Typical manufacturing
Cm - Nital Etched Micrography by OMDf - At the Surface