Crevice Corrosion in a Subsea System — Aspect Before Analysis
Microstructure — sub-branches
Aligned particles 1Alpha and Beta 2Clad Interface 4Delta ferrite 1Ferrite and Pearlite 3Fusion Line 4Granular structure 1Graphite in Flakes 1Graphite in Imperfect Nodules 1Graphite in Nodules 1Intragranular Secondary Precipitation 1Martensite 8Non Metallic Inclusions 1Pearlite 2Sigma 4Strain Hardened 1Zn Layer 2

ML00178 / Jan.2022
Cold cracks in Cr-Mo Welded Forging
M - CrMo SteelP - ForgingAp - O&G Well DrillingCd - Welding Defect
Cm - Nital Etched Micrography by SEMDf - Fusion Line
ML00163 / Jun.2020
Corrosion Fatigue of a Boiler Waterwall Tube
M - Low Carbon SteelP - Seamless tubeAp - BoilerCd - Corrosion Fatigue
Cm - Nital Etched Micrography by SEMDf - Pearlite

ML00154 / Jan.2019
High Strength Cast Iron Crankshaft
M - Nodular Cast IronP - CastingAp - EngineCd - Surface treatment
Cm - Nital Etched Micrography by SEMDf - Graphite in Nodules

ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Micrography by SEMDf - Granular structure

ML00144 / Aug.2018
Impact of a .380 Winchester on Ti64 Plate
M - Ti6Al4VP - Rolled PlateAp - StructureCd - Non-Pierced
Cm - Micrography by SEMDf - Alpha and Beta

ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - Nital Etched Micrography by SEMDf - Ferrite and Pearlite

ML00142 / Aug.2018
Impact of a .308 Winchester on AR500 Plate
M - Low Alloy Wear ResistantP - Rolled PlateAp - StructureCd - Non-Pierced
Cm - Nital Etched Micrography by SEMDf - Martensite

ML00141 / Jul.2018
Brittle Fracture of a Corroded Gray Cast Iron
M - Gray Cast ironP - CastingAp - EngineCd - Brittle Fracture
Cm - Nital Etched Micrography by SEMDf - Graphite in Flakes
More from these cases

ML00154 / Jan.2019
High Strength Cast Iron Crankshaft
M - Nodular Cast IronP - CastingAp - EngineCd - Surface treatment
Cm - Nital Etched Micrography by SEMDf - Ferrite and Pearlite

ML00154 / Jan.2019
High Strength Cast Iron Crankshaft
M - Nodular Cast IronP - CastingAp - EngineCd - Surface treatment
Cm - Nital Etched Micrography by SEMDf - Pearlite

ML00154 / Jan.2019
High Strength Cast Iron Crankshaft
M - Nodular Cast IronP - CastingAp - EngineCd - Surface treatment
Cm - Nital Etched Micrography by SEMDf - Graphite in Imperfect Nodules

ML00154 / Jan.2019
High Strength Cast Iron Crankshaft
M - Nodular Cast IronP - CastingAp - EngineCd - Surface treatment
Cm - Nital Etched Micrography by SEMDf - Martensite

ML00154 / Jan.2019
High Strength Cast Iron Crankshaft
M - Nodular Cast IronP - CastingAp - EngineCd - Surface treatment
Cm - Nital Etched Micrography by SEMDf - Martensite

ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Micrography by SEMDf - Aligned particles

ML00144 / Aug.2018
Impact of a .380 Winchester on Ti64 Plate
M - Ti6Al4VP - Rolled PlateAp - StructureCd - Non-Pierced
Cm - Micrography by SEMDf - Alpha and Beta

ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - Nital Etched Micrography by SEMDf - Ferrite and Pearlite

ML00142 / Aug.2018
Impact of a .308 Winchester on AR500 Plate
M - Low Alloy Wear ResistantP - Rolled PlateAp - StructureCd - Non-Pierced
Cm - Nital Etched Micrography by SEMDf - Martensite