Microstructure

93 cases · 324 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00184 / Apr.2023
Dissimilar Steels in a Threaded Connection
M - Low Carbon SteelP - ForgingAp - OffshoreCd - Localized Dissolution
Cm - Nital Etched Micrography by OMDf - Bainitic Ferrite
ML00183 / Dec.2022
Ductile Behavior of an Aluminum Wheel
M - Aluminum Silicon MagnesiumP - CastingAp - AutomotiveCd - Ductile Behavior
Cm - Keller Etched Micrography by OMDf - Hypoeutetic
Tempered martensitic structure for the F22 forging base metal.
129
ML00178 / Jan.2022
Cold cracks in Cr-Mo Welded Forging
M - CrMo SteelP - ForgingAp - O&G Well DrillingCd - Welding Defect
Cm - Nital Etched Micrography by OMDf - Tempered Martensite
ML00177 / Dec.2021
Cr-Mo Seam Welded Tube
M - CrMo SteelP - Longitudinally Seam WeldedAp - Fired HeaterCd - Not according to spec
Cm - Nital Etched Micrography by OMDf - Granular structure
ML00170 / Sep.2020
MIC in Aluminum Brass Tubes
M - Aluminum BrassP - Seamless tubeAp - MaritimeCd - Preferential Dissolution
Cm - FeCl3+HCl+Ethanol Etched MicroDf - Alpha
Micrography of the tranverse section of the tube, in the center of the thickness.  There are small grains and large grains, characterizing a dual grain size.  The large grains size is about 100 microns, more than 10 times larger than the average size of the smaller grains size.
101
ML00165 / Jul.2020
SCC of Aluminum Bronze Heating Coil
M - Aluminum BronzeP - Seamless tubeAp - Oil and GasCd - Stress Corrosion
Cm - FeCl3+HCl+H2O Etched MicroDf - Dual grain sizes
The tube microstructure is ferritic-pearlitic, typical of this kind of material.  No evidences of microstrutural changes were detected (no overheating, no decarburization).
177
ML00163 / Jun.2020
Corrosion Fatigue of a Boiler Waterwall Tube
M - Low Carbon SteelP - Seamless tubeAp - BoilerCd - Corrosion Fatigue
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite
ML00164 / Jun.2020
Austenitic SS Casting for Valve Body
M - Austenitic Stainless SteelP - CastingAp - ValveCd - Typical manufacturing
Cm - Oxalic Acid Electrolytic EtchDf - Austenite

More from these cases

ML00183 — Ductile Behavior of an Aluminum WheelM - Aluminum Silicon MagnesiumP - CastingAp - AutomotiveCd - Ductile Behavior
ML00183 / Dec.2022
Ductile Behavior of an Aluminum Wheel
M - Aluminum Silicon MagnesiumP - CastingAp - AutomotiveCd - Ductile Behavior
Cm - Keller Etched Micrography by OMDf - Networklike precipitates
ML00178 — Cold cracks in Cr-Mo Welded ForgingM - CrMo SteelP - ForgingAp - O&G Well DrillingCd - Welding Defect
ML00178 / Jan.2022
Cold cracks in Cr-Mo Welded Forging
M - CrMo SteelP - ForgingAp - O&G Well DrillingCd - Welding Defect
Cm - Nital Etched Micrography by OMDf - Martensite
ML00178 / Jan.2022
Cold cracks in Cr-Mo Welded Forging
M - CrMo SteelP - ForgingAp - O&G Well DrillingCd - Welding Defect
Cm - Nital Etched Micrography by OMDf - Tempered Martensite
ML00178 / Jan.2022
Cold cracks in Cr-Mo Welded Forging
M - CrMo SteelP - ForgingAp - O&G Well DrillingCd - Welding Defect
Cm - Nital Etched Micrography by OMDf - Tempered Martensite
ML00177 — Cr-Mo Seam Welded TubeM - CrMo SteelP - Longitudinally Seam WeldedAp - Fired HeaterCd - Not according to spec
ML00177 / Dec.2021
Cr-Mo Seam Welded Tube
M - CrMo SteelP - Longitudinally Seam WeldedAp - Fired HeaterCd - Not according to spec
Cm - Nital Etched Micrography by OMDf - Grain refined structure
ML00177 / Dec.2021
Cr-Mo Seam Welded Tube
M - CrMo SteelP - Longitudinally Seam WeldedAp - Fired HeaterCd - Not according to spec
Cm - Nital Etched Micrography by OMDf - Bainitic HAZ
ML00177 / Dec.2021
Cr-Mo Seam Welded Tube
M - CrMo SteelP - Longitudinally Seam WeldedAp - Fired HeaterCd - Not according to spec
Cm - Nital Etched Micrography by OMDf - Ferrite and Bainite
ML00177 / Dec.2021
Cr-Mo Seam Welded Tube
M - CrMo SteelP - Longitudinally Seam WeldedAp - Fired HeaterCd - Not according to spec
Cm - Nital Etched Micrography by OMDf - Bainitic HAZ
ML00177 / Dec.2021
Cr-Mo Seam Welded Tube
M - CrMo SteelP - Longitudinally Seam WeldedAp - Fired HeaterCd - Not according to spec
Cm - Nital Etched Micrography by OMDf - Bainite

+1 more from this case →

ML00170 — MIC in Aluminum Brass TubesM - Aluminum BrassP - Seamless tubeAp - MaritimeCd - Preferential Dissolution
ML00170 / Sep.2020
MIC in Aluminum Brass Tubes
M - Aluminum BrassP - Seamless tubeAp - MaritimeCd - Preferential Dissolution
Cm - FeCl3+HCl+Ethanol Etched MicroDf - Alpha
ML00165 — SCC of Aluminum Bronze Heating CoilM - Aluminum BronzeP - Seamless tubeAp - Oil and GasCd - Stress Corrosion
ML00165 / Jul.2020
SCC of Aluminum Bronze Heating Coil
M - Aluminum BronzeP - Seamless tubeAp - Oil and GasCd - Stress Corrosion
Cm - FeCl3+HCl+H2O Etched MicroDf - Alpha
ML00164 — Austenitic SS Casting for Valve BodyM - Austenitic Stainless SteelP - CastingAp - ValveCd - Typical manufacturing
ML00164 / Jun.2020
Austenitic SS Casting for Valve Body
M - Austenitic Stainless SteelP - CastingAp - ValveCd - Typical manufacturing
Cm - Oxalic Acid Electrolytic EtchDf - Delta ferrite
ML00164 / Jun.2020
Austenitic SS Casting for Valve Body
M - Austenitic Stainless SteelP - CastingAp - ValveCd - Typical manufacturing
Cm - Oxalic Acid Electrolytic EtchDf - Delta ferrite
ML00164 / Jun.2020
Austenitic SS Casting for Valve Body
M - Austenitic Stainless SteelP - CastingAp - ValveCd - Typical manufacturing
Cm - Oxalic Acid Electrolytic EtchDf - Austenite
ML00164 / Jun.2020
Austenitic SS Casting for Valve Body
M - Austenitic Stainless SteelP - CastingAp - ValveCd - Typical manufacturing
Cm - Oxalic Acid Electrolytic EtchDf - Delta ferrite
ML00164 / Jun.2020
Austenitic SS Casting for Valve Body
M - Austenitic Stainless SteelP - CastingAp - ValveCd - Typical manufacturing
Cm - Oxalic Acid Electrolytic EtchDf - Delta ferrite