Predominantly Ferritic
6 cases · 15 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00112 / Dec.2017
1" XXS Pipe Not Qualified For Low Temp
M - Low Carbon SteelP - Seamless PipeAp - RefineryCd - Not according to spec
Cm - Nital Etched Micrography by OMDf - Predominantly Ferritic

ML00103 / Nov.2017
Brittle Fracture of a Free-Cutting Connector
M - Low Carbon SteelP - Machined PartAp - ShipCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Predominantly Ferritic

ML00083 / Oct.2017
Steel Back of a Bimetallic Engine Bearing
M - Low Carbon SteelP - Cold FormedAp - ShipCd - Removed From Service
Cm - Nital Etched Micrography by OMDf - Predominantly Ferritic

ML00047 / Mar.2017
Ductile Cast Iron Caps of Electrical Insulators
M - Ductile Cast IronP - Cast iron capAp - EnergyCd - Typical manufacturing
Cm - Nital Etched Micrography by OMDf - Predominantly Ferritic

ML00034 / Apr.2017
45 Years Old Acquaduct Grey Cast Iron
M - Gray Cast ironP - Centrifugally Cast PipeAp - AcquaductCd - General Corrosion
Cm - Nital Etched Micrography by OMDf - Predominantly Ferritic Matrix

ML00001 / Dec.2017
Thermal Fatigue of Cast Iron
M - Nodular Cast IronP - CastAp - SiderurgyCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Predominantly Ferritic Matrix
More from these cases

ML00112 / Dec.2017
1" XXS Pipe Not Qualified For Low Temp
M - Low Carbon SteelP - Seamless PipeAp - RefineryCd - Not according to spec
Cm - Nital Etched Micrography by OMDf - Predominantly Ferritic

ML00112 / Dec.2017
1" XXS Pipe Not Qualified For Low Temp
M - Low Carbon SteelP - Seamless PipeAp - RefineryCd - Not according to spec
Cm - Nital Etched Micrography by OMDf - Predominantly Ferritic

ML00047 / Mar.2017
Ductile Cast Iron Caps of Electrical Insulators
M - Ductile Cast IronP - Cast iron capAp - EnergyCd - Typical manufacturing
Cm - Nital Etched Micrography by OMDf - Predominantly Ferritic

ML00047 / Mar.2017
Ductile Cast Iron Caps of Electrical Insulators
M - Ductile Cast IronP - Cast iron capAp - EnergyCd - Typical manufacturing
Cm - Nital Etched Micrography by OMDf - Predominantly Ferritic

ML00034 / Apr.2017
45 Years Old Acquaduct Grey Cast Iron
M - Gray Cast ironP - Centrifugally Cast PipeAp - AcquaductCd - General Corrosion
Cm - Nital Etched Micrography by OMDf - Predominantly Ferritic Matrix

ML00034 / Apr.2017
45 Years Old Acquaduct Grey Cast Iron
M - Gray Cast ironP - Centrifugally Cast PipeAp - AcquaductCd - General Corrosion
Cm - Nital Etched Micrography by OMDf - Predominantly Ferritic Matrix

ML00034 / Apr.2017
45 Years Old Acquaduct Grey Cast Iron
M - Gray Cast ironP - Centrifugally Cast PipeAp - AcquaductCd - General Corrosion
Cm - Nital Etched Micrography by OMDf - Predominantly Ferritic Matrix

ML00034 / Apr.2017
45 Years Old Acquaduct Grey Cast Iron
M - Gray Cast ironP - Centrifugally Cast PipeAp - AcquaductCd - General Corrosion
Cm - Nital Etched Micrography by OMDf - Predominantly Ferritic Matrix

ML00034 / Apr.2017
45 Years Old Acquaduct Grey Cast Iron
M - Gray Cast ironP - Centrifugally Cast PipeAp - AcquaductCd - General Corrosion
Cm - Nital Etched Micrography by OMDf - Predominantly Ferritic Matrix