Pearlite

3 cases · 7 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00175 / Aug.2021
Localized External Wear of a Wire Rope
M - High Carbon SteelP - Wire RopeAp - Oil and GasCd - Wear
Cm - Nital Etched Micrography by OMDf - Pearlite
ML00158 / Feb.2020
Surface Hardened Carbon Steel Wheel
M - High Carbon SteelP - WheelAp - TransportationCd - Removed From Service
Cm - Nital Etched Micrography by OMDf - Pearlite
Micrographic detail of a transverse section of the rail, in the head, showing a fully perlitic structure.
520
ML00096 / Oct.2017
Carbon Steel Tee Rail
M - High Strength Low AlloyP - RailAp - TransportationCd - Typical manufacturing
Cm - Nital Etched Micrography by OMDf - Pearlite

More from these cases

ML00175 — Localized External Wear of a Wire RopeM - High Carbon SteelP - Wire RopeAp - Oil and GasCd - Wear
ML00175 / Aug.2021
Localized External Wear of a Wire Rope
M - High Carbon SteelP - Wire RopeAp - Oil and GasCd - Wear
Cm - Nital Etched Micrography by OMDf - Pearlite
ML00158 — Surface Hardened Carbon Steel WheelM - High Carbon SteelP - WheelAp - TransportationCd - Removed From Service
ML00158 / Feb.2020
Surface Hardened Carbon Steel Wheel
M - High Carbon SteelP - WheelAp - TransportationCd - Removed From Service
Cm - Nital Etched Micrography by OMDf - Pearlite
ML00158 / Feb.2020
Surface Hardened Carbon Steel Wheel
M - High Carbon SteelP - WheelAp - TransportationCd - Removed From Service
Cm - Nital Etched Micrography by OMDf - Pearlite
ML00096 — Carbon Steel Tee RailM - High Strength Low AlloyP - RailAp - TransportationCd - Typical manufacturing
ML00096 / Oct.2017
Carbon Steel Tee Rail
M - High Strength Low AlloyP - RailAp - TransportationCd - Typical manufacturing
Cm - Nital Etched Micrography by OMDf - Perlite