Coalesced structure

2 cases · 6 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00119 / Feb.2018
Thermal Fatigue of a Marine Boiler
M - Low Carbon SteelP - Fabrication WeldAp - ShipCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Coalesced structure
Micrography of a longitudinal section of the tube, at the cracked region, in the center of the thickness,  showing an evolution of the perlitic structure into carbides.
110
ML00104 / Dec.2017
Thermal Fatigue of a Boiler Tube
M - Low Carbon SteelP - Autogenously Welded TubeAp - BoilerCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Coalesced structure

More from these cases

ML00119 — Thermal Fatigue of a Marine BoilerM - Low Carbon SteelP - Fabrication WeldAp - ShipCd - Thermal Fatigue
ML00119 / Feb.2018
Thermal Fatigue of a Marine Boiler
M - Low Carbon SteelP - Fabrication WeldAp - ShipCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Coalesced structure
ML00104 — Thermal Fatigue of a Boiler TubeM - Low Carbon SteelP - Autogenously Welded TubeAp - BoilerCd - Thermal Fatigue
Micrographic detail of a longitudinal section of the tube, at the cracked region, in the center of the thickness. The pearlitic structure was already degratated into globular carbides.
101
ML00104 / Dec.2017
Thermal Fatigue of a Boiler Tube
M - Low Carbon SteelP - Autogenously Welded TubeAp - BoilerCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Coalesced structure
ML00104 / Dec.2017
Thermal Fatigue of a Boiler Tube
M - Low Carbon SteelP - Autogenously Welded TubeAp - BoilerCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Coalesced structure
ML00104 / Dec.2017
Thermal Fatigue of a Boiler Tube
M - Low Carbon SteelP - Autogenously Welded TubeAp - BoilerCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Coalesced structure