Austenite

10 cases · 17 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00164 / Jun.2020
Austenitic SS Casting for Valve Body
M - Austenitic Stainless SteelP - CastingAp - ValveCd - Typical manufacturing
Cm - Oxalic Acid Electrolytic EtchDf - Austenite
Low magnification micrography, by optical microscope, of the longitudinal section of a damaged bolt, in the center of the thickness. The microstructure is austenitic, free from carbides.
100
ML00157 / Feb.2020
Bolts Under Chloride SCC Conditions
M - Austenitic Stainless SteelP - BoltAp - Oil and GasCd - Stress Corrosion
Cm - Oxalic Acid Electrolytic EtchDf - Austenite
Nitronic 60 cylinder. Micrography of the longitudinal section in the center of the thickness, presenting a fully austenitic microstructure, equiaxial grains, and evidences of the manufacturing process by hot forming.
179
ML00121 / Feb.2018
Pitting Corrosion in a Subsea System
M - Austenitic / MartensiticP - Rod & CylinderAp - SubseaCd - Pitting Corrosion
Cm - Micrography by OM using A262 Method ADf - Austenite
Micrographic detail of the strain hardened austenitic structure in the longitudinal section of the bolt.
441
ML00101 / Nov.2017
High Strength 316SS Bolt
M - Austenitic Stainless SteelP - BoltAp - SubseaCd - Typical manufacturing
Cm - Micrography by OM using A262 Method ADf - Austenite
Micrographic detail of the strain hardened austenitic structure in the longitudinal section of the bolt.
412
ML00087 / Nov.2017
High Strength Austenitic SS Bolt
M - Austenitic Stainless SteelP - BoltAp - SubseaCd - Typical manufacturing
Cm - Micrography by OM using A262 Method ADf - Austenite
Micrography of the 1.65 mm thickness tube, in the middle of the thickness of the longitudinal section.  This part of the tube is located in the colder part of the equipment, position 1.  The material presented carbide precipitation at grain boundaries (not yet fully surrounding the grains) and at this point the tube presented no internal corrosion.
338
ML00086 / Nov.2017
Intergranular Corrosion of Sensitized 304SS
M - Austenitic Stainless SteelP - Seamless tubeAp - Heat ExchangerCd - Intergranular Corrosion
Cm - Micrography by OM using A262 Method ADf - Austenite
ML00056 / May.2018
Seamless Tube Externally Cladded with SS
M - Carbon Steel / Stainless SteelP - CladdingAp - Pulp and PaperCd - Removed From Service
Cm - Micrography by OM using A262 Method ADf - Austenite
The shell plate micrography showed an austenitic structure.
101
ML00050 / Nov.2017
Fatigue Failure of a 316SS Pressure Stabilizer
M - Austenitic Stainless SteelP - Fabrication WeldAp - Chemical IndustryCd - Mechanical Fatigue
Cm - Micrography by OM using A262 Method ADf - Austenite

More from these cases

ML00164 — Austenitic SS Casting for Valve BodyM - Austenitic Stainless SteelP - CastingAp - ValveCd - Typical manufacturing
ML00164 / Jun.2020
Austenitic SS Casting for Valve Body
M - Austenitic Stainless SteelP - CastingAp - ValveCd - Typical manufacturing
Cm - Oxalic Acid Electrolytic EtchDf - Austenite
ML00121 — Pitting Corrosion in a Subsea SystemM - Austenitic / MartensiticP - Rod & CylinderAp - SubseaCd - Pitting Corrosion
Nitronic 60 cylinder. Micrography of the longitudinal section in the center of the thickness, presenting a fully austenitic microstructure, with some aligned non metallic inclusions.
157
ML00121 / Feb.2018
Pitting Corrosion in a Subsea System
M - Austenitic / MartensiticP - Rod & CylinderAp - SubseaCd - Pitting Corrosion
Cm - Micrography by OM using A262 Method ADf - Austenite
Nitronic 60 cylinder. Micrographic detail of the longitudinal section in the center of the thickness, presenting a fully austenitic microstructure, equiaxial grains, typical of a solution annealed condition.
136
ML00121 / Feb.2018
Pitting Corrosion in a Subsea System
M - Austenitic / MartensiticP - Rod & CylinderAp - SubseaCd - Pitting Corrosion
Cm - Micrography by OM using A262 Method ADf - Austenite
ML00101 — High Strength 316SS BoltM - Austenitic Stainless SteelP - BoltAp - SubseaCd - Typical manufacturing
ML00101 / Nov.2017
High Strength 316SS Bolt
M - Austenitic Stainless SteelP - BoltAp - SubseaCd - Typical manufacturing
Cm - Micrography by OM using A262 Method ADf - Austenite
ML00087 — High Strength Austenitic SS BoltM - Austenitic Stainless SteelP - BoltAp - SubseaCd - Typical manufacturing
ML00087 / Nov.2017
High Strength Austenitic SS Bolt
M - Austenitic Stainless SteelP - BoltAp - SubseaCd - Typical manufacturing
Cm - Micrography by OM using A262 Method ADf - Austenite