1 case · 1 image
Crevice Corrosion in a Subsea System — Aspect Before Analysis
Atlas
/
Detail focus
/
Sampling and Analysis
/ External Surface
Product: Forging
×
Condition: Welding Defect
×
Capture method: Aspect Before Analysis
×
clear all
Results
Sort
Newest
Oldest
Title A-Z
Title Z-A
165
VIEW
ML00178 / Jan.2022
Cold cracks in Cr-Mo Welded Forging
M
- CrMo Steel
P
- Forging
Ap
- O&G Well Drilling
Cd
- Welding Defect
Cm
- Aspect Before Analysis
Df
- External Surface