ML00144 / Aug.2018
Impact of a .380 Winchester on Ti64 Plate
M - Ti6Al4VP - Rolled PlateAp - StructureCd - Non-Pierced
Cm - Micrography by SEMDf - Melted film
More from these cases

ML00144 / Aug.2018
Impact of a .380 Winchester on Ti64 Plate
M - Ti6Al4VP - Rolled PlateAp - StructureCd - Non-Pierced
Cm - Micrography by SEMDf - Plastic Deformation

ML00144 / Aug.2018
Impact of a .380 Winchester on Ti64 Plate
M - Ti6Al4VP - Rolled PlateAp - StructureCd - Non-Pierced
Cm - Micrography by SEMDf - Plastic Deformation

ML00144 / Aug.2018
Impact of a .380 Winchester on Ti64 Plate
M - Ti6Al4VP - Rolled PlateAp - StructureCd - Non-Pierced
Cm - Micrography by SEMDf - Plastic Deformation

ML00144 / Aug.2018
Impact of a .380 Winchester on Ti64 Plate
M - Ti6Al4VP - Rolled PlateAp - StructureCd - Non-Pierced
Cm - Micrography by SEMDf - Dimples

ML00144 / Aug.2018
Impact of a .380 Winchester on Ti64 Plate
M - Ti6Al4VP - Rolled PlateAp - StructureCd - Non-Pierced