Localized Corrosion

4 cases · 7 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00135 / May.2018
MIC of a Non Magnetic Drilling Tool
M - High Mn Austenitic SteelP - Tubular ForgingAp - O&G Well DrillingCd - Pitting Corrosion
Cm - Surface Aspect by SEMDf - Localized Corrosion
Scanning electron microscopy image of the chromium plated cylinder surface, presenting deposits and localized dissolution under deposits. There are different stages of corrosion in this region, observed in low magnification. Small areas of attack and a shallow pitting with deposits that were analyzed by EDS and revealed the presence of S.
903
ML00128 / Apr.2018
MIC of a Stored Hydraulic Cylinder
M - Low Carbon SteelP - Chromium PlatedAp - OffshoreCd - Localized Dissolution
Cm - Surface Aspect by SEMDf - Localized Corrosion
Nitronic 60 cylinder. Scanning electron microscopy image of a corroded region at the external surface of the cylinder, that is austenitic.  The image shows the localized corroded regions in form of pits.
1228
ML00121 / Feb.2018
Pitting Corrosion in a Subsea System
M - Austenitic / MartensiticP - Rod & CylinderAp - SubseaCd - Pitting Corrosion
Cm - Surface Aspect by SEMDf - Localized Corrosion
Regions of the pin thread presenting pitting corrosion.
635
ML00016 / Apr.2017
SCC in Free Cutting 303SS
M - Austenitic Stainless SteelP - Machined PartAp - OffshoreCd - Stress Corrosion
Cm - Surface Aspect by SEMDf - Localized Corrosion

More from these cases

ML00121 — Pitting Corrosion in a Subsea SystemM - Austenitic / MartensiticP - Rod & CylinderAp - SubseaCd - Pitting Corrosion
Nitronic 60 cylinder. Scanning electron microscopy image of a corroded region at the external surface of the cylinder, that is austenitic.  The image shows the structure revealed by dissolution of the material (inside the pits) evidencing the strain hardened layer that is presented at the cylinder surface due to the manufacturing process.
106
ML00121 / Feb.2018
Pitting Corrosion in a Subsea System
M - Austenitic / MartensiticP - Rod & CylinderAp - SubseaCd - Pitting Corrosion
Cm - Surface Aspect by SEMDf - Localized Corrosion
Nitronic 60 cylinder. Scanning electron microscopy image detail of a corroded region inside a pitting showing the etched structure (strain hardened austenitic structure).
103
ML00121 / Feb.2018
Pitting Corrosion in a Subsea System
M - Austenitic / MartensiticP - Rod & CylinderAp - SubseaCd - Pitting Corrosion
Cm - Surface Aspect by SEMDf - Localized Corrosion
ML00121 / Feb.2018
Pitting Corrosion in a Subsea System
M - Austenitic / MartensiticP - Rod & CylinderAp - SubseaCd - Pitting Corrosion
Cm - Surface Aspect by SEMDf - Localized Corrosion