Damage

12 cases · 144 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Micrography of a transverse section of the platesheet presenting a duplex structure, alpha (light yellow) and beta (orange) phases.
214
ML00125 / Mar.2018
Dezincification of a Cooler Tubesheet
M - BrassP - PlateAp - ShipCd - Preferential Dissolution
Cm - FeCl3+HCl+Ethanol Etched MicroDf - Alpha and Beta
Micrography of the plate in a longitudinal section, presenting a typical ferritic pearlitic structure, banded.  The plate is 22 mm thick.
182
ML00119 / Feb.2018
Thermal Fatigue of a Marine Boiler
M - Low Carbon SteelP - Fabrication WeldAp - ShipCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Banded Structure
ML00103 / Nov.2017
Brittle Fracture of a Free-Cutting Connector
M - Low Carbon SteelP - Machined PartAp - ShipCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Longitudinal Section
The cast iron microstructure is predominatly ferritic with graphite nodules.
169
ML00040 / Apr.2017
Brittle Fracture of a Valve Stem
M - Nodular Cast IronP - Valve StemAp - ShipCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Graphite in Nodules

More from these cases

ML00125 — Dezincification of a Cooler TubesheetM - BrassP - PlateAp - ShipCd - Preferential Dissolution
Micrography of the transverse section of the platesheet at the interface between the corroded and the non-corroded regions. The micrography is in the as polished condition.
140
ML00125 / Mar.2018
Dezincification of a Cooler Tubesheet
M - BrassP - PlateAp - ShipCd - Preferential Dissolution
Cm - As polished micrographyDf - Preferential Dissolution
Micrography of the transverse section of the platesheet showing that part of the material (right side in the top of the figure) was lost (corroded).
129
ML00125 / Mar.2018
Dezincification of a Cooler Tubesheet
M - BrassP - PlateAp - ShipCd - Preferential Dissolution
Cm - As polished micrographyDf - Preferential Dissolution
Micrographic detail of the dezincification effect, where the beta phase is preferentially corroded, leaving a cooper rich phase (red) that is porous and easily cracks.
121
ML00125 / Mar.2018
Dezincification of a Cooler Tubesheet
M - BrassP - PlateAp - ShipCd - Preferential Dissolution
Cm - As polished micrographyDf - Dezincification
Micrographic detail of the dezincification effect, where the beta phase is preferentially corroded, leaving a cooper rich phase (red) that is porous and easily cracks.
130
ML00125 / Mar.2018
Dezincification of a Cooler Tubesheet
M - BrassP - PlateAp - ShipCd - Preferential Dissolution
Cm - As polished micrographyDf - Cracks
Micrography showing detachment of material at the surface of the platesheet. The cracks are associated to the dezincification effect, where the beta phase was preferentially corroded and became a weak porous layer.
113
ML00125 / Mar.2018
Dezincification of a Cooler Tubesheet
M - BrassP - PlateAp - ShipCd - Preferential Dissolution
Cm - As polished micrographyDf - Crack

+7 more from this case →

ML00119 — Thermal Fatigue of a Marine BoilerM - Low Carbon SteelP - Fabrication WeldAp - ShipCd - Thermal Fatigue
Micrography of the plate in a longitudinal section, presenting a typical ferritic pearlitic structure, banded.
165
ML00119 / Feb.2018
Thermal Fatigue of a Marine Boiler
M - Low Carbon SteelP - Fabrication WeldAp - ShipCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite
Micrographic detail of the ferritic pearlitic structure of the plate in the longitudinal section.
147
ML00119 / Feb.2018
Thermal Fatigue of a Marine Boiler
M - Low Carbon SteelP - Fabrication WeldAp - ShipCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite
Micrography of the weld metal in the center os the weld. Columnar grains (of the previous austenite) with primary ferrite in the grain boundaries; ferrite with aligned second phases and acicular ferrite, intragranular.
137
ML00119 / Feb.2018
Thermal Fatigue of a Marine Boiler
M - Low Carbon SteelP - Fabrication WeldAp - ShipCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Weld Metal
Micrography of the weld metal in the center os the weld. Columnar grains (of the previous austenite) with primary ferrite in the grain boundaries and acicular ferrite intragranular.
125
ML00119 / Feb.2018
Thermal Fatigue of a Marine Boiler
M - Low Carbon SteelP - Fabrication WeldAp - ShipCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Ferritic Weld Metal
Micrographic detail of the weld metal in the center os the weld. Columnar grains (of the previous austenite) with primary ferrite in the grain boundaries; and details of the ferrite with aligned second phases and acicular ferrite, intragranular.
112
ML00119 / Feb.2018
Thermal Fatigue of a Marine Boiler
M - Low Carbon SteelP - Fabrication WeldAp - ShipCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Ferritic Weld Metal

+12 more from this case →

ML00103 — Brittle Fracture of a Free-Cutting ConnectorM - Low Carbon SteelP - Machined PartAp - ShipCd - Brittle Fracture
Micrographic detail of the longitudinal section of the fitiing, in a free-cutting steel.  The microstructure is predominantly ferritic, with small perlitic areas and some free cementite at ferritic grain boundaries.  There is a large amount of sulfide inclusions, aligned perpendicular to the forming direction.
107
ML00103 / Nov.2017
Brittle Fracture of a Free-Cutting Connector
M - Low Carbon SteelP - Machined PartAp - ShipCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Non Metallic Inclusions
ML00103 / Nov.2017
Brittle Fracture of a Free-Cutting Connector
M - Low Carbon SteelP - Machined PartAp - ShipCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Transverse Section
ML00103 / Nov.2017
Brittle Fracture of a Free-Cutting Connector
M - Low Carbon SteelP - Machined PartAp - ShipCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Predominantly Ferritic
ML00103 / Nov.2017
Brittle Fracture of a Free-Cutting Connector
M - Low Carbon SteelP - Machined PartAp - ShipCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Crack
ML00103 / Nov.2017
Brittle Fracture of a Free-Cutting Connector
M - Low Carbon SteelP - Machined PartAp - ShipCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Crack

+4 more from this case →

ML00040 — Brittle Fracture of a Valve StemM - Nodular Cast IronP - Valve StemAp - ShipCd - Brittle Fracture
The micrography of the stem at the fracture region shows a flat fracture with transgranular clevage at the ferritic structure.
137
ML00040 / Apr.2017
Brittle Fracture of a Valve Stem
M - Nodular Cast IronP - Valve StemAp - ShipCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Fracture
Micrography presenting a detail of the fracture surface opening to the graphite nodules.
139
ML00040 / Apr.2017
Brittle Fracture of a Valve Stem
M - Nodular Cast IronP - Valve StemAp - ShipCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Fracture