Surface Aspect by SEM

12 cases · 39 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00170 / Sep.2020
MIC in Aluminum Brass Tubes
M - Aluminum BrassP - Seamless tubeAp - MaritimeCd - Preferential Dissolution
Cm - Surface Aspect by SEMDf - Internal Surface
ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Surface Aspect by SEMDf - Plastic Deformation
ML00144 / Aug.2018
Impact of a .380 Winchester on Ti64 Plate
M - Ti6Al4VP - Rolled PlateAp - StructureCd - Non-Pierced
Cm - Surface Aspect by SEMDf - Melted film
ML00125 / Mar.2018
Dezincification of a Cooler Tubesheet
M - BrassP - PlateAp - ShipCd - Preferential Dissolution
Cm - Surface Aspect by SEMDf - Corrosion
Microscopic image by scanning electron microscope (SEM) of the ring surface that presented pites under fouling deposits.
522
ML00124 / Feb.2018
MIC of a Martensitic Valve Ring
M - Martensitic Stainless SteelP - ForgingAp - EnergyCd - Brittle Behavior
Cm - Surface Aspect by SEMDf - Pitting
The scanning electron microscopy image of the internal surface of the tube in position 2 shows a localized  corrosion region with intergranular morphology, as well a crack from the corroded region.
1237
ML00086 / Nov.2017
Intergranular Corrosion of Sensitized 304SS
M - Austenitic Stainless SteelP - Seamless tubeAp - Heat ExchangerCd - Intergranular Corrosion
Cm - Surface Aspect by SEMDf - Intergranular Corrosion
ML00012 / Aug.2017
Vibration Induced Fatigue in a 316/316L SS
M - Austenitic Stainless SteelP - Seamless PipeAp - OffshoreCd - Vibration Induced Fatigue
Cm - Surface Aspect by SEMDf - External Surface
Aspect of the rusted surface after cleaning, showing adhered products at the surface, in regions where the passive layer was destroyed and pitting corrosion occurred.
184
ML00054 / Dec.2018
Cutlery Corrosion
M - Martensitic Stainless SteelP - Foodstuff ArticleAp - KitchenCd - Pitting Corrosion
Cm - Surface Aspect by SEMDf - Corrosion

More from these cases

ML00170 — MIC in Aluminum Brass TubesM - Aluminum BrassP - Seamless tubeAp - MaritimeCd - Preferential Dissolution
ML00170 / Sep.2020
MIC in Aluminum Brass Tubes
M - Aluminum BrassP - Seamless tubeAp - MaritimeCd - Preferential Dissolution
Cm - Surface Aspect by SEMDf - Pitting
ML00170 / Sep.2020
MIC in Aluminum Brass Tubes
M - Aluminum BrassP - Seamless tubeAp - MaritimeCd - Preferential Dissolution
Cm - Surface Aspect by SEMDf - Corrosion
ML00145 — Impact of a .380 Winchester on 6061 T6 PlateM - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Surface Aspect by SEMDf - At the Surface
ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Surface Aspect by SEMDf - At the Surface
ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Surface Aspect by SEMDf - At the Surface
ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Surface Aspect by SEMDf - Ductile Fracture
ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Surface Aspect by SEMDf - At the Surface
ML00144 — Impact of a .380 Winchester on Ti64 PlateM - Ti6Al4VP - Rolled PlateAp - StructureCd - Non-Pierced
ML00144 / Aug.2018
Impact of a .380 Winchester on Ti64 Plate
M - Ti6Al4VP - Rolled PlateAp - StructureCd - Non-Pierced
Cm - Surface Aspect by SEMDf - Melted film
ML00144 / Aug.2018
Impact of a .380 Winchester on Ti64 Plate
M - Ti6Al4VP - Rolled PlateAp - StructureCd - Non-Pierced
Cm - Surface Aspect by SEMDf - Melted film
ML00144 / Aug.2018
Impact of a .380 Winchester on Ti64 Plate
M - Ti6Al4VP - Rolled PlateAp - StructureCd - Non-Pierced
Cm - Surface Aspect by SEMDf - Melted film
ML00144 / Aug.2018
Impact of a .380 Winchester on Ti64 Plate
M - Ti6Al4VP - Rolled PlateAp - StructureCd - Non-Pierced
Cm - Surface Aspect by SEMDf - Melted film
ML00144 / Aug.2018
Impact of a .380 Winchester on Ti64 Plate
M - Ti6Al4VP - Rolled PlateAp - StructureCd - Non-Pierced
Cm - Surface Aspect by SEMDf - Melted film

+3 more from this case →

ML00124 — MIC of a Martensitic Valve RingM - Martensitic Stainless SteelP - ForgingAp - EnergyCd - Brittle Behavior
ML00124 / Feb.2018
MIC of a Martensitic Valve Ring
M - Martensitic Stainless SteelP - ForgingAp - EnergyCd - Brittle Behavior
Cm - Surface Aspect by SEMDf - Pitting
ML00124 / Feb.2018
MIC of a Martensitic Valve Ring
M - Martensitic Stainless SteelP - ForgingAp - EnergyCd - Brittle Behavior
Cm - Surface Aspect by SEMDf - Pitting
ML00124 / Feb.2018
MIC of a Martensitic Valve Ring
M - Martensitic Stainless SteelP - ForgingAp - EnergyCd - Brittle Behavior
Cm - Surface Aspect by SEMDf - Pitting
ML00124 / Feb.2018
MIC of a Martensitic Valve Ring
M - Martensitic Stainless SteelP - ForgingAp - EnergyCd - Brittle Behavior
Cm - Surface Aspect by SEMDf - Pitting
ML00086 — Intergranular Corrosion of Sensitized 304SSM - Austenitic Stainless SteelP - Seamless tubeAp - Heat ExchangerCd - Intergranular Corrosion
The low magnification image of the internal surface of the tube, in position 2, shows several points of localized corrosion, with intergranular morphology.
193
ML00086 / Nov.2017
Intergranular Corrosion of Sensitized 304SS
M - Austenitic Stainless SteelP - Seamless tubeAp - Heat ExchangerCd - Intergranular Corrosion
Cm - Surface Aspect by SEMDf - Intergranular Corrosion
ML00012 — Vibration Induced Fatigue in a 316/316L SSM - Austenitic Stainless SteelP - Seamless PipeAp - OffshoreCd - Vibration Induced Fatigue
ML00012 / Aug.2017
Vibration Induced Fatigue in a 316/316L SS
M - Austenitic Stainless SteelP - Seamless PipeAp - OffshoreCd - Vibration Induced Fatigue
Cm - Surface Aspect by SEMDf - Pitting
ML00054 — Cutlery CorrosionM - Martensitic Stainless SteelP - Foodstuff ArticleAp - KitchenCd - Pitting Corrosion
Detail of the rusted surface. EDS analysis inside the pitting shows a high Cl peak (the bright aspect inside the pitting), indicating that the salt over the surface was responsible for destroying the passive layer and the localized corrosion occurred.
172
ML00054 / Dec.2018
Cutlery Corrosion
M - Martensitic Stainless SteelP - Foodstuff ArticleAp - KitchenCd - Pitting Corrosion
Cm - Surface Aspect by SEMDf - Corrosion