Fractography by SEM

1 case · 4 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Fractographic aspect of the broken fastener, at the surface, showing na intergranular morphology typical of a hydrogen assisted mechanism of a high strenght steel under cathodic protection.
224
ML00074 / Jun.2018
Hydrogen Cracking of a 17-4 PH Subsea Bolt
M - Precipitation Hardened Stainless SteelP - FastenerAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Intergranular Cracking

More from these cases

ML00074 — Hydrogen Cracking of a 17-4 PH Subsea BoltM - Precipitation Hardened Stainless SteelP - FastenerAp - SubseaCd - Hydrogen Embrittlement
Microscopic aspect of the fracture, close to the bolt surface where the fracture is macroscopically brittle, presenting a predominantly intergranular fracture micromechanism.
108
ML00074 / Jun.2018
Hydrogen Cracking of a 17-4 PH Subsea Bolt
M - Precipitation Hardened Stainless SteelP - FastenerAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Brittle Fracture
ML00074 / Jun.2018
Hydrogen Cracking of a 17-4 PH Subsea Bolt
M - Precipitation Hardened Stainless SteelP - FastenerAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Brittle Fracture
ML00074 / Jun.2018
Hydrogen Cracking of a 17-4 PH Subsea Bolt
M - Precipitation Hardened Stainless SteelP - FastenerAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Ductile Fracture