ML00141 / Jul.2018
Brittle Fracture of a Corroded Gray Cast Iron
M
- Gray Cast iron
P
- Casting
Ap
- Engine
Cd
- Brittle Fracture
Cm
- Fractography by SEM
Df
- Close to the External Surface