Fractography by SEM

3 cases · 4 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00167 / Aug.2020
Fatigue of a Flared Tubing Connection
M - Austenitic Stainless SteelP - TubingAp - EngineCd - Mechanical Fatigue
Cm - Fractography by SEMDf - Close to the External Surface
ML00141 / Jul.2018
Brittle Fracture of a Corroded Gray Cast Iron
M - Gray Cast ironP - CastingAp - EngineCd - Brittle Fracture
Cm - Fractography by SEMDf - Close to the External Surface
ML00131 / Apr.2018
Brittle Failure of a Soft Roller Bearing
M - Wear Resistant SteelP - Roller BearingAp - Mechanical IndustryCd - Heat Treatment Defect
Cm - Fractography by SEMDf - Close to the External Surface

More from these cases

ML00131 — Brittle Failure of a Soft Roller BearingM - Wear Resistant SteelP - Roller BearingAp - Mechanical IndustryCd - Heat Treatment Defect
ML00131 / Apr.2018
Brittle Failure of a Soft Roller Bearing
M - Wear Resistant SteelP - Roller BearingAp - Mechanical IndustryCd - Heat Treatment Defect
Cm - Fractography by SEMDf - Close to the External Surface