Optical Microscope

3 cases · 27 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Micrography of a crankshaft longitudinal section at the shaft edge, in the as polished condition, presenting nodular graphite, well distruibuted.
139
ML00154 / Jan.2019
High Strength Cast Iron Crankshaft
M - Nodular Cast IronP - CastingAp - EngineCd - Surface treatment
Cm - As polished micrographyDf - At the Surface
Micrography of CAP A, showing graphite in imperfect nodules and ferritic matrix.
481
ML00047 / Mar.2017
Ductile Cast Iron Caps of Electrical Insulators
M - Ductile Cast IronP - Cast iron capAp - EnergyCd - Typical manufacturing
Cm - Nital Etched Micrography by OMDf - Graphite in Imperfect Nodules
The cast iron microstructure is predominatly ferritic with graphite nodules.
169
ML00040 / Apr.2017
Brittle Fracture of a Valve Stem
M - Nodular Cast IronP - Valve StemAp - ShipCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Graphite in Nodules

More from these cases

ML00154 — High Strength Cast Iron CrankshaftM - Nodular Cast IronP - CastingAp - EngineCd - Surface treatment
As polished micrography of the crankshaft at the shaft edge, close to the surface.  Graphite in nodules.
126
ML00154 / Jan.2019
High Strength Cast Iron Crankshaft
M - Nodular Cast IronP - CastingAp - EngineCd - Surface treatment
Cm - As polished micrographyDf - Graphite in Nodules
As polished micrographic detail of the graphite in nodules, close to the surface of the shaft edge, in a longitudinal section.
114
ML00154 / Jan.2019
High Strength Cast Iron Crankshaft
M - Nodular Cast IronP - CastingAp - EngineCd - Surface treatment
Cm - As polished micrographyDf - Graphite in Nodules
ML00154 / Jan.2019
High Strength Cast Iron Crankshaft
M - Nodular Cast IronP - CastingAp - EngineCd - Surface treatment
Cm - Nital Etched Micrography by OMDf - At the Surface
ML00154 / Jan.2019
High Strength Cast Iron Crankshaft
M - Nodular Cast IronP - CastingAp - EngineCd - Surface treatment
Cm - Nital Etched Micrography by OMDf - Matrix of ferrite and pearlite
ML00154 / Jan.2019
High Strength Cast Iron Crankshaft
M - Nodular Cast IronP - CastingAp - EngineCd - Surface treatment
Cm - Nital Etched Micrography by OMDf - Matrix of ferrite and pearlite

+12 more from this case →

ML00047 — Ductile Cast Iron Caps of Electrical InsulatorsM - Ductile Cast IronP - Cast iron capAp - EnergyCd - Typical manufacturing
ML00047 / Mar.2017
Ductile Cast Iron Caps of Electrical Insulators
M - Ductile Cast IronP - Cast iron capAp - EnergyCd - Typical manufacturing
Cm - Nital Etched Micrography by OMDf - Predominantly Ferritic
ML00047 / Mar.2017
Ductile Cast Iron Caps of Electrical Insulators
M - Ductile Cast IronP - Cast iron capAp - EnergyCd - Typical manufacturing
Cm - Nital Etched Micrography by OMDf - Graphite in Nodules
ML00047 / Mar.2017
Ductile Cast Iron Caps of Electrical Insulators
M - Ductile Cast IronP - Cast iron capAp - EnergyCd - Typical manufacturing
Cm - Nital Etched Micrography by OMDf - Predominantly Ferritic
ML00047 / Mar.2017
Ductile Cast Iron Caps of Electrical Insulators
M - Ductile Cast IronP - Cast iron capAp - EnergyCd - Typical manufacturing
Cm - Nital Etched Micrography by OMDf - Graphite in Nodules
ML00047 / Mar.2017
Ductile Cast Iron Caps of Electrical Insulators
M - Ductile Cast IronP - Cast iron capAp - EnergyCd - Typical manufacturing
Cm - Nital Etched Micrography by OMDf - Predominantly Ferritic
ML00040 — Brittle Fracture of a Valve StemM - Nodular Cast IronP - Valve StemAp - ShipCd - Brittle Fracture
The micrography of the stem at the fracture region shows a flat fracture with transgranular clevage at the ferritic structure.
137
ML00040 / Apr.2017
Brittle Fracture of a Valve Stem
M - Nodular Cast IronP - Valve StemAp - ShipCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Fracture
Micrography presenting a detail of the fracture surface opening to the graphite nodules.
139
ML00040 / Apr.2017
Brittle Fracture of a Valve Stem
M - Nodular Cast IronP - Valve StemAp - ShipCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Fracture