Kalling Etched Micrography by OM
7 cases · 56 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Kalling Etched Micrography by OMDf - Martensite

ML00124 / Feb.2018
MIC of a Martensitic Valve Ring
M - Martensitic Stainless SteelP - ForgingAp - EnergyCd - Brittle Behavior
Cm - Kalling Etched Micrography by OMDf - Martensite

ML00121 / Feb.2018
Pitting Corrosion in a Subsea System
M - Austenitic / MartensiticP - Rod & CylinderAp - SubseaCd - Pitting Corrosion
Cm - Kalling Etched Micrography by OMDf - Martensite

ML00085 / Nov.2017
Corrosion Fatigue of a Martensitic SS Pin
M - Martensitic Stainless SteelP - Forged PinAp - O&G Well DrillingCd - Corrosion Fatigue
Cm - Kalling Etched Micrography by OMDf - Martensite

ML00065 / May.2017
Erosion Corrosion of Monel Piping
M - NiCu AlloyP - Seamless PipeAp - Chemical IndustryCd - Erosion Corrosion
Cm - Kalling Etched Micrography by OMDf - Base Metal Left Side

ML00054 / Dec.2018
Cutlery Corrosion
M - Martensitic Stainless SteelP - Foodstuff ArticleAp - KitchenCd - Pitting Corrosion
Cm - Kalling Etched Micrography by OMDf - Pitting

ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Kalling Etched Micrography by OMDf - Austenite
More from these cases

ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Kalling Etched Micrography by OMDf - Intergranular Cracking

ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Kalling Etched Micrography by OMDf - Intergranular Cracking

ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Kalling Etched Micrography by OMDf - Intergranular Cracking

ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Kalling Etched Micrography by OMDf - Intergranular Fracture

ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Kalling Etched Micrography by OMDf - Intergranular Fracture

ML00124 / Feb.2018
MIC of a Martensitic Valve Ring
M - Martensitic Stainless SteelP - ForgingAp - EnergyCd - Brittle Behavior
Cm - Kalling Etched Micrography by OMDf - Martensite

ML00124 / Feb.2018
MIC of a Martensitic Valve Ring
M - Martensitic Stainless SteelP - ForgingAp - EnergyCd - Brittle Behavior
Cm - Kalling Etched Micrography by OMDf - Crack

ML00124 / Feb.2018
MIC of a Martensitic Valve Ring
M - Martensitic Stainless SteelP - ForgingAp - EnergyCd - Brittle Behavior
Cm - Kalling Etched Micrography by OMDf - Intergranular Cracking

ML00124 / Feb.2018
MIC of a Martensitic Valve Ring
M - Martensitic Stainless SteelP - ForgingAp - EnergyCd - Brittle Behavior
Cm - Kalling Etched Micrography by OMDf - Crack

ML00124 / Feb.2018
MIC of a Martensitic Valve Ring
M - Martensitic Stainless SteelP - ForgingAp - EnergyCd - Brittle Behavior
Cm - Kalling Etched Micrography by OMDf - Crack

ML00121 / Feb.2018
Pitting Corrosion in a Subsea System
M - Austenitic / MartensiticP - Rod & CylinderAp - SubseaCd - Pitting Corrosion
Cm - Kalling Etched Micrography by OMDf - Martensite

ML00121 / Feb.2018
Pitting Corrosion in a Subsea System
M - Austenitic / MartensiticP - Rod & CylinderAp - SubseaCd - Pitting Corrosion
Cm - Kalling Etched Micrography by OMDf - Martensite

ML00121 / Feb.2018
Pitting Corrosion in a Subsea System
M - Austenitic / MartensiticP - Rod & CylinderAp - SubseaCd - Pitting Corrosion
Cm - Kalling Etched Micrography by OMDf - Pitting

ML00085 / Nov.2017
Corrosion Fatigue of a Martensitic SS Pin
M - Martensitic Stainless SteelP - Forged PinAp - O&G Well DrillingCd - Corrosion Fatigue
Cm - Kalling Etched Micrography by OMDf - Banded Structure

ML00085 / Nov.2017
Corrosion Fatigue of a Martensitic SS Pin
M - Martensitic Stainless SteelP - Forged PinAp - O&G Well DrillingCd - Corrosion Fatigue
Cm - Kalling Etched Micrography by OMDf - Martensite

ML00085 / Nov.2017
Corrosion Fatigue of a Martensitic SS Pin
M - Martensitic Stainless SteelP - Forged PinAp - O&G Well DrillingCd - Corrosion Fatigue
Cm - Kalling Etched Micrography by OMDf - Fracture

ML00085 / Nov.2017
Corrosion Fatigue of a Martensitic SS Pin
M - Martensitic Stainless SteelP - Forged PinAp - O&G Well DrillingCd - Corrosion Fatigue
Cm - Kalling Etched Micrography by OMDf - Fracture

ML00085 / Nov.2017
Corrosion Fatigue of a Martensitic SS Pin
M - Martensitic Stainless SteelP - Forged PinAp - O&G Well DrillingCd - Corrosion Fatigue
Cm - Kalling Etched Micrography by OMDf - Fatigue Fracture

ML00065 / May.2017
Erosion Corrosion of Monel Piping
M - NiCu AlloyP - Seamless PipeAp - Chemical IndustryCd - Erosion Corrosion
Cm - Kalling Etched Micrography by OMDf - Base Metal Left Side

ML00065 / May.2017
Erosion Corrosion of Monel Piping
M - NiCu AlloyP - Seamless PipeAp - Chemical IndustryCd - Erosion Corrosion
Cm - Kalling Etched Micrography by OMDf - Base Metal Right Side

ML00065 / May.2017
Erosion Corrosion of Monel Piping
M - NiCu AlloyP - Seamless PipeAp - Chemical IndustryCd - Erosion Corrosion
Cm - Kalling Etched Micrography by OMDf - Base Metal Right Side

ML00065 / May.2017
Erosion Corrosion of Monel Piping
M - NiCu AlloyP - Seamless PipeAp - Chemical IndustryCd - Erosion Corrosion
Cm - Kalling Etched Micrography by OMDf - Fusion Line Left Side

ML00065 / May.2017
Erosion Corrosion of Monel Piping
M - NiCu AlloyP - Seamless PipeAp - Chemical IndustryCd - Erosion Corrosion
Cm - Kalling Etched Micrography by OMDf - Fusion Line Left Side

ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Kalling Etched Micrography by OMDf - Austenite

ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Kalling Etched Micrography by OMDf - Austenite

ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Kalling Etched Micrography by OMDf - Corrosion Cracking

ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Kalling Etched Micrography by OMDf - Corrosion Cracking