Crevice Corrosion in a Subsea System — Aspect Before Analysis
Condition: Preferential Dissolution ×Standard: UNS ×Capture method: Naked Eye or Stereoscope ×clear all

ML00125 / Mar.2018
Dezincification of a Cooler Tubesheet
M - BrassP - PlateAp - ShipCd - Preferential Dissolution
Cm - Surface AspectDf - Corrosion
More from these cases

ML00125 / Mar.2018
Dezincification of a Cooler Tubesheet
M - BrassP - PlateAp - ShipCd - Preferential Dissolution
Cm - Transverse Section AspectDf - Corrosion

ML00125 / Mar.2018
Dezincification of a Cooler Tubesheet
M - BrassP - PlateAp - ShipCd - Preferential Dissolution
Cm - Transverse Section AspectDf - Corrosion

ML00125 / Mar.2018
Dezincification of a Cooler Tubesheet
M - BrassP - PlateAp - ShipCd - Preferential Dissolution
Cm - Transverse Section AspectDf - Dezincification