Atlas

11 cases · 26 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Fractography by SEMDf - Intergranular Fracture
ML00160 / Apr.2020
High Temperature Degradation of 310SS
M - Austenitic Stainless SteelP - Rectangular TubeAp - Chemical IndustryCd - Scaling
Cm - Oxalic Acid Electrolytic EtchDf - Intergranular Fracture
ML00148 / Sep.2018
Brittle Fracture of a 420 SS Barrel Nut
M - Martensitic Stainless SteelP - Barrel NutAp - LiftingCd - Heat Treatment Defect
Cm - Fractography by SEMDf - Intergranular Fracture
ML00139 / Jun.2018
Hydrogen Fracture of a 17-4 PH Allen Bolt
M - Precipitation Hardened Stainless SteelP - Allen BoltAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Intergranular Fracture
ML00138 / Jun.2018
Liquid Metal Embrittlement of a HSLA Steel
M - High Strength Low AlloyP - Coated ProductAp - Mechanical IndustryCd - Liquid Metal Embrittlement
Cm - Fractography by SEMDf - Intergranular Fracture
ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Fractography by SEMDf - Intergranular Fracture
ML00127 / May.2018
Hydrogen Cracks of Cadmium Plated Studs
M - Low Alloy Medium Carbon QTP - Allen StudAp - Oil and GasCd - Hydrogen Embrittlement
Cm - Nital Etched Micrography by OMDf - Intergranular Fracture
Aspect of the fracture surface of the bolt, after cleaning with a  plastic brush.  Although there is a layer of oxides it is possible to see the intergranular morphology of the fracture, typical of a hydrogen embrittlement mechanism.
1154
ML00126 / Mar.2018
Hydrogen Fracture of Subsea Allen Bolts
M - Low Alloy Medium Carbon QTP - Coated ProductAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Intergranular Fracture

More from these cases

ML00182 — Brittle Fracture of a LAS Fixing RodM - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Fractography by SEMDf - Intergranular Fracture
ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Fractography by SEMDf - Intergranular Fracture
ML00160 — High Temperature Degradation of 310SSM - Austenitic Stainless SteelP - Rectangular TubeAp - Chemical IndustryCd - Scaling
ML00160 / Apr.2020
High Temperature Degradation of 310SS
M - Austenitic Stainless SteelP - Rectangular TubeAp - Chemical IndustryCd - Scaling
Cm - As polished micrographyDf - Intergranular Fracture
ML00148 — Brittle Fracture of a 420 SS Barrel NutM - Martensitic Stainless SteelP - Barrel NutAp - LiftingCd - Heat Treatment Defect
ML00148 / Sep.2018
Brittle Fracture of a 420 SS Barrel Nut
M - Martensitic Stainless SteelP - Barrel NutAp - LiftingCd - Heat Treatment Defect
Cm - Kalling Etched Micrography by OMDf - Intergranular Fracture
ML00139 — Hydrogen Fracture of a 17-4 PH Allen BoltM - Precipitation Hardened Stainless SteelP - Allen BoltAp - SubseaCd - Hydrogen Embrittlement
ML00139 / Jun.2018
Hydrogen Fracture of a 17-4 PH Allen Bolt
M - Precipitation Hardened Stainless SteelP - Allen BoltAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Intergranular Fracture
ML00139 / Jun.2018
Hydrogen Fracture of a 17-4 PH Allen Bolt
M - Precipitation Hardened Stainless SteelP - Allen BoltAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Intergranular Fracture
ML00138 — Liquid Metal Embrittlement of a HSLA SteelM - High Strength Low AlloyP - Coated ProductAp - Mechanical IndustryCd - Liquid Metal Embrittlement
ML00138 / Jun.2018
Liquid Metal Embrittlement of a HSLA Steel
M - High Strength Low AlloyP - Coated ProductAp - Mechanical IndustryCd - Liquid Metal Embrittlement
Cm - Fractography by SEMDf - Intergranular Fracture
ML00137 — Brittle Fracture of a 15-5 PH Valve SpringM - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Fractography by SEMDf - Intergranular Fracture
ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Kalling Etched Micrography by OMDf - Intergranular Fracture
ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Kalling Etched Micrography by OMDf - Intergranular Fracture
ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Kalling Etched Micrography by OMDf - Intergranular Fracture
ML00126 — Hydrogen Fracture of Subsea Allen BoltsM - Low Alloy Medium Carbon QTP - Coated ProductAp - SubseaCd - Hydrogen Embrittlement
Detailed aspect of the fracture surface of the bolt, evidencing the intergranular morphology of the fracture (although with an oxide scale), typical of a hydrogen embrittlement mechanism.
114
ML00126 / Mar.2018
Hydrogen Fracture of Subsea Allen Bolts
M - Low Alloy Medium Carbon QTP - Coated ProductAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Intergranular Fracture