Atlas

30 cases · 97 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00144 / Aug.2018
Impact of a .380 Winchester on Ti64 Plate
M - Ti6Al4VP - Rolled PlateAp - StructureCd - Non-Pierced
Cm - Surface Aspect by SEMDf - Melted film
ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - Surface Aspect by SEMDf - Plastic Deformation
ML00142 / Aug.2018
Impact of a .308 Winchester on AR500 Plate
M - Low Alloy Wear ResistantP - Rolled PlateAp - StructureCd - Non-Pierced
Cm - Surface Aspect by SEMDf - Low Mag
ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Surface Aspect by SEMDf - Corrosion
Microscopical aspect by scanning electron microscopy (SEM) of the external surface of a drilling tool in a position that presented localized deposits and corrosion under deposit. The deep corrosion in a short time is only possible associated to the biological growth and aggressive environment generated by the microorganisms metabolites - Microbiologically Induced Corrosion (MIC).
104
ML00135 / May.2018
MIC of a Non Magnetic Drilling Tool
M - High Mn Austenitic SteelP - Tubular ForgingAp - O&G Well DrillingCd - Pitting Corrosion
Cm - Surface Aspect by SEMDf - Localized Deposits
Scanning electron microscopy image of the chromium plated cylinder surface, presenting deposits and localized dissolution under deposits. There are different stages of corrosion in this region, observed in low magnification. Small areas of attack and a shallow pitting with deposits that were analyzed by EDS and revealed the presence of S.
903
ML00128 / Apr.2018
MIC of a Stored Hydraulic Cylinder
M - Low Carbon SteelP - Chromium PlatedAp - OffshoreCd - Localized Dissolution
Cm - Surface Aspect by SEMDf - Localized Corrosion
ML00125 / Mar.2018
Dezincification of a Cooler Tubesheet
M - BrassP - PlateAp - ShipCd - Preferential Dissolution
Cm - Surface Aspect by SEMDf - Corrosion
Microscopic image by scanning electron microscope (SEM) of the ring surface that presented pites under fouling deposits.
522
ML00124 / Feb.2018
MIC of a Martensitic Valve Ring
M - Martensitic Stainless SteelP - ForgingAp - EnergyCd - Brittle Behavior
Cm - Surface Aspect by SEMDf - Pitting

More from these cases

ML00144 — Impact of a .380 Winchester on Ti64 PlateM - Ti6Al4VP - Rolled PlateAp - StructureCd - Non-Pierced
ML00144 / Aug.2018
Impact of a .380 Winchester on Ti64 Plate
M - Ti6Al4VP - Rolled PlateAp - StructureCd - Non-Pierced
Cm - Surface Aspect by SEMDf - Melted film
ML00144 / Aug.2018
Impact of a .380 Winchester on Ti64 Plate
M - Ti6Al4VP - Rolled PlateAp - StructureCd - Non-Pierced
Cm - Surface Aspect by SEMDf - Melted film
ML00144 / Aug.2018
Impact of a .380 Winchester on Ti64 Plate
M - Ti6Al4VP - Rolled PlateAp - StructureCd - Non-Pierced
Cm - Surface Aspect by SEMDf - Melted film
ML00144 / Aug.2018
Impact of a .380 Winchester on Ti64 Plate
M - Ti6Al4VP - Rolled PlateAp - StructureCd - Non-Pierced
Cm - Surface Aspect by SEMDf - Melted film
ML00144 / Aug.2018
Impact of a .380 Winchester on Ti64 Plate
M - Ti6Al4VP - Rolled PlateAp - StructureCd - Non-Pierced
Cm - Surface Aspect by SEMDf - Melted film

+3 more from this case →

ML00143 — Impact of a .308 Winchester on A36 PlateM - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - Surface Aspect by SEMDf - At the Surface
ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - Surface Aspect by SEMDf - At the Surface
ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - Surface Aspect by SEMDf - At the Surface
ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - Surface Aspect by SEMDf - Dimples
ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - Surface Aspect by SEMDf - Melted film
ML00142 — Impact of a .308 Winchester on AR500 PlateM - Low Alloy Wear ResistantP - Rolled PlateAp - StructureCd - Non-Pierced
ML00142 / Aug.2018
Impact of a .308 Winchester on AR500 Plate
M - Low Alloy Wear ResistantP - Rolled PlateAp - StructureCd - Non-Pierced
Cm - Surface Aspect by SEMDf - At the Surface
ML00142 / Aug.2018
Impact of a .308 Winchester on AR500 Plate
M - Low Alloy Wear ResistantP - Rolled PlateAp - StructureCd - Non-Pierced
Cm - Surface Aspect by SEMDf - At the Surface
ML00142 / Aug.2018
Impact of a .308 Winchester on AR500 Plate
M - Low Alloy Wear ResistantP - Rolled PlateAp - StructureCd - Non-Pierced
Cm - Surface Aspect by SEMDf - At the Surface
ML00142 / Aug.2018
Impact of a .308 Winchester on AR500 Plate
M - Low Alloy Wear ResistantP - Rolled PlateAp - StructureCd - Non-Pierced
Cm - Surface Aspect by SEMDf - At the Surface
ML00137 — Brittle Fracture of a 15-5 PH Valve SpringM - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Surface Aspect by SEMDf - Corrosion
ML00135 — MIC of a Non Magnetic Drilling ToolM - High Mn Austenitic SteelP - Tubular ForgingAp - O&G Well DrillingCd - Pitting Corrosion
ML00135 / May.2018
MIC of a Non Magnetic Drilling Tool
M - High Mn Austenitic SteelP - Tubular ForgingAp - O&G Well DrillingCd - Pitting Corrosion
Cm - Surface Aspect by SEMDf - Localized Corrosion
ML00128 — MIC of a Stored Hydraulic CylinderM - Low Carbon SteelP - Chromium PlatedAp - OffshoreCd - Localized Dissolution
ML00128 / Apr.2018
MIC of a Stored Hydraulic Cylinder
M - Low Carbon SteelP - Chromium PlatedAp - OffshoreCd - Localized Dissolution
Cm - Surface Aspect by SEMDf - At the Surface
ML00128 / Apr.2018
MIC of a Stored Hydraulic Cylinder
M - Low Carbon SteelP - Chromium PlatedAp - OffshoreCd - Localized Dissolution
Cm - Surface Aspect by SEMDf - Corrosion
ML00128 / Apr.2018
MIC of a Stored Hydraulic Cylinder
M - Low Carbon SteelP - Chromium PlatedAp - OffshoreCd - Localized Dissolution
Cm - Surface Aspect by SEMDf - Corrosion
ML00124 — MIC of a Martensitic Valve RingM - Martensitic Stainless SteelP - ForgingAp - EnergyCd - Brittle Behavior
ML00124 / Feb.2018
MIC of a Martensitic Valve Ring
M - Martensitic Stainless SteelP - ForgingAp - EnergyCd - Brittle Behavior
Cm - Surface Aspect by SEMDf - Pitting
ML00124 / Feb.2018
MIC of a Martensitic Valve Ring
M - Martensitic Stainless SteelP - ForgingAp - EnergyCd - Brittle Behavior
Cm - Surface Aspect by SEMDf - Pitting
ML00124 / Feb.2018
MIC of a Martensitic Valve Ring
M - Martensitic Stainless SteelP - ForgingAp - EnergyCd - Brittle Behavior
Cm - Surface Aspect by SEMDf - Pitting
ML00124 / Feb.2018
MIC of a Martensitic Valve Ring
M - Martensitic Stainless SteelP - ForgingAp - EnergyCd - Brittle Behavior
Cm - Surface Aspect by SEMDf - Pitting