Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00176 / Nov.2021
Hydride Formation in a Titanium Blade
M - Unalloyed TitaniumP - BladeAp - Oil and GasCd - Hydride Formation
Cm - Fractography by SEMDf - Cleavage Facets
ML00139 / Jun.2018
Hydrogen Fracture of a 17-4 PH Allen Bolt
M - Precipitation Hardened Stainless SteelP - Allen BoltAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Cleavage Facets
ML00134 / Aug.2020
Brittle Fracture of a Superduplex Valve Body
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Fracture
Cm - Fractography by SEMDf - Cleavage Facets
ML00103 / Nov.2017
Brittle Fracture of a Free-Cutting Connector
M - Low Carbon SteelP - Machined PartAp - ShipCd - Brittle Fracture
Cm - Fractography by SEMDf - Cleavage Facets
ML00088 / Dec.2017
Hydrogen Cracking of an API 5D S135 Drill Pipe
M - Low Alloy Medium Carbon QTP - Drill PipeAp - SubseaCd - Hydrogen Embrittlement
Cm - Surface Aspect by SEMDf - Cleavage Facets
The fracture surface is flat, shows the graphite nodules and cleavage of the ferritic microstructure, indicating that the material have exceeded the capacity to acomodate the stress.
944
ML00040 / Apr.2017
Brittle Fracture of a Valve Stem
M - Nodular Cast IronP - Valve StemAp - ShipCd - Brittle Fracture
Cm - Fractography by SEMDf - Cleavage Facets
The fracture surface, although presenting a large amount of corrosion products, shows also evidences of a brittle behavior with regions of cleavage micromechanism.
116
ML00002 / Jan.2018
Preferential Dissolution and Cracks in SDSS
M - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Cm - Fractography by SEMDf - Cleavage Facets

More from these cases

ML00176 — Hydride Formation in a Titanium BladeM - Unalloyed TitaniumP - BladeAp - Oil and GasCd - Hydride Formation
ML00176 / Nov.2021
Hydride Formation in a Titanium Blade
M - Unalloyed TitaniumP - BladeAp - Oil and GasCd - Hydride Formation
Cm - Fractography by SEMDf - Cleavage Facets
ML00139 — Hydrogen Fracture of a 17-4 PH Allen BoltM - Precipitation Hardened Stainless SteelP - Allen BoltAp - SubseaCd - Hydrogen Embrittlement
ML00139 / Jun.2018
Hydrogen Fracture of a 17-4 PH Allen Bolt
M - Precipitation Hardened Stainless SteelP - Allen BoltAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Cleavage Facets
ML00134 — Brittle Fracture of a Superduplex Valve BodyM - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Fracture
ML00134 / Aug.2020
Brittle Fracture of a Superduplex Valve Body
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Fracture
Cm - Fractography by SEMDf - Cleavage Facets
ML00040 — Brittle Fracture of a Valve StemM - Nodular Cast IronP - Valve StemAp - ShipCd - Brittle Fracture
Detail of the cleavage micromechanism.
195
ML00040 / Apr.2017
Brittle Fracture of a Valve Stem
M - Nodular Cast IronP - Valve StemAp - ShipCd - Brittle Fracture
Cm - Fractography by SEMDf - Cleavage Facets
ML00002 — Preferential Dissolution and Cracks in SDSSM - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
ML00002 / Jan.2018
Preferential Dissolution and Cracks in SDSS
M - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Cm - Fractography by SEMDf - Cleavage Facets
ML00002 / Jan.2018
Preferential Dissolution and Cracks in SDSS
M - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Cm - Fractography by SEMDf - Cleavage Facets