Atlas

4 cases · 7 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00160 / Apr.2020
High Temperature Degradation of 310SS
M - Austenitic Stainless SteelP - Rectangular TubeAp - Chemical IndustryCd - Scaling
Cm - Oxalic Acid Electrolytic EtchDf - Intergranular Fracture
ML00148 / Sep.2018
Brittle Fracture of a 420 SS Barrel Nut
M - Martensitic Stainless SteelP - Barrel NutAp - LiftingCd - Heat Treatment Defect
Cm - Kalling Etched Micrography by OMDf - Intergranular Fracture
ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Kalling Etched Micrography by OMDf - Intergranular Fracture
ML00127 / May.2018
Hydrogen Cracks of Cadmium Plated Studs
M - Low Alloy Medium Carbon QTP - Allen StudAp - Oil and GasCd - Hydrogen Embrittlement
Cm - Nital Etched Micrography by OMDf - Intergranular Fracture

More from these cases

ML00160 — High Temperature Degradation of 310SSM - Austenitic Stainless SteelP - Rectangular TubeAp - Chemical IndustryCd - Scaling
ML00160 / Apr.2020
High Temperature Degradation of 310SS
M - Austenitic Stainless SteelP - Rectangular TubeAp - Chemical IndustryCd - Scaling
Cm - As polished micrographyDf - Intergranular Fracture
ML00137 — Brittle Fracture of a 15-5 PH Valve SpringM - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Kalling Etched Micrography by OMDf - Intergranular Fracture
ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Kalling Etched Micrography by OMDf - Intergranular Fracture