Atlas
49 cases · 166 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00183 / Dec.2022
Ductile Behavior of an Aluminum Wheel
M - Aluminum Silicon MagnesiumP - CastingAp - AutomotiveCd - Ductile Behavior
Cm - Fractography by SEMDf - General View

ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Fractography by SEMDf - Intergranular Fracture

ML00181 / Apr.2022
Wear of a Carburized Hypoid Gear
M - Low Alloy for Thermochemical TreatmentP - Pinion-crown assemblyAp - ShipCd - Wear
Cm - Fractography by SEMDf - Fatigue Fracture

ML00179 / Feb.2022
Hydrides in Titanium Weld
M - Unalloyed TitaniumP - In Field WeldAp - Chemical IndustryCd - Hydride Formation
Cm - Fractography by SEMDf - Fracture

ML00176 / Nov.2021
Hydride Formation in a Titanium Blade
M - Unalloyed TitaniumP - BladeAp - Oil and GasCd - Hydride Formation
Cm - Fractography by SEMDf - Fracture

ML00174 / Jul.2021
Carburization of a 347 SS Welded Joint
M - Austenitic Stainless SteelP - Fabrication WeldAp - EnergyCd - Carburization
Cm - Fractography by SEMDf - Brittle Fracture

ML00171 / Feb.2021
Corrosion Fatigue of U Bolt Pipe Clamp
M - Low Carbon SteelP - BoltAp - ShipCd - Corrosion Fatigue
Cm - Fractography by SEMDf - Fracture

ML00167 / Aug.2020
Fatigue of a Flared Tubing Connection
M - Austenitic Stainless SteelP - TubingAp - EngineCd - Mechanical Fatigue
Cm - Fractography by SEMDf - Fracture
More from these cases

ML00183 / Dec.2022
Ductile Behavior of an Aluminum Wheel
M - Aluminum Silicon MagnesiumP - CastingAp - AutomotiveCd - Ductile Behavior
Cm - Fractography by SEMDf - Ductile Fracture

ML00183 / Dec.2022
Ductile Behavior of an Aluminum Wheel
M - Aluminum Silicon MagnesiumP - CastingAp - AutomotiveCd - Ductile Behavior
Cm - Fractography by SEMDf - Elongated Dimples

ML00183 / Dec.2022
Ductile Behavior of an Aluminum Wheel
M - Aluminum Silicon MagnesiumP - CastingAp - AutomotiveCd - Ductile Behavior
Cm - Fractography by SEMDf - Cracks

ML00183 / Dec.2022
Ductile Behavior of an Aluminum Wheel
M - Aluminum Silicon MagnesiumP - CastingAp - AutomotiveCd - Ductile Behavior
Cm - Fractography by SEMDf - Cracks

ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Fractography by SEMDf - Intergranular Fracture

ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Fractography by SEMDf - Intergranular Fracture

ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Fractography by SEMDf - Broken Testpiece

ML00182 / Jul.2022
Brittle Fracture of a LAS Fixing Rod
M - Low Alloy Medium Carbon QTP - StemAp - Mechanical IndustryCd - Brittle Fracture
Cm - Fractography by SEMDf - Broken Testpiece

ML00179 / Feb.2022
Hydrides in Titanium Weld
M - Unalloyed TitaniumP - In Field WeldAp - Chemical IndustryCd - Hydride Formation
Cm - Fractography by SEMDf - Brittle Cracks

ML00179 / Feb.2022
Hydrides in Titanium Weld
M - Unalloyed TitaniumP - In Field WeldAp - Chemical IndustryCd - Hydride Formation
Cm - Fractography by SEMDf - Secondary Cracks

ML00179 / Feb.2022
Hydrides in Titanium Weld
M - Unalloyed TitaniumP - In Field WeldAp - Chemical IndustryCd - Hydride Formation
Cm - Fractography by SEMDf - Fatigue Striation

ML00176 / Nov.2021
Hydride Formation in a Titanium Blade
M - Unalloyed TitaniumP - BladeAp - Oil and GasCd - Hydride Formation
Cm - Fractography by SEMDf - Cleavage Facets

ML00176 / Nov.2021
Hydride Formation in a Titanium Blade
M - Unalloyed TitaniumP - BladeAp - Oil and GasCd - Hydride Formation
Cm - Fractography by SEMDf - Cleavage Facets

ML00174 / Jul.2021
Carburization of a 347 SS Welded Joint
M - Austenitic Stainless SteelP - Fabrication WeldAp - EnergyCd - Carburization
Cm - Fractography by SEMDf - Brittle Fracture

ML00167 / Aug.2020
Fatigue of a Flared Tubing Connection
M - Austenitic Stainless SteelP - TubingAp - EngineCd - Mechanical Fatigue
Cm - Fractography by SEMDf - Close to the External Surface

ML00167 / Aug.2020
Fatigue of a Flared Tubing Connection
M - Austenitic Stainless SteelP - TubingAp - EngineCd - Mechanical Fatigue
Cm - Fractography by SEMDf - Fatigue Fracture

ML00167 / Aug.2020
Fatigue of a Flared Tubing Connection
M - Austenitic Stainless SteelP - TubingAp - EngineCd - Mechanical Fatigue
Cm - Fractography by SEMDf - Fatigue Striation

ML00167 / Aug.2020
Fatigue of a Flared Tubing Connection
M - Austenitic Stainless SteelP - TubingAp - EngineCd - Mechanical Fatigue
Cm - Fractography by SEMDf - Fatigue Striation

ML00167 / Aug.2020
Fatigue of a Flared Tubing Connection
M - Austenitic Stainless SteelP - TubingAp - EngineCd - Mechanical Fatigue
Cm - Fractography by SEMDf - Fatigue Fracture