Crevice Corrosion in a Subsea System — Aspect Before Analysis
Application: FPSO ×Condition: Pitting Corrosion ×Capture method: Scanning Electron Microscope ×clear all

ML00014 / Apr.2017
Pitting Corrosion in 316SS Pipe
M - Austenitic Stainless SteelP - Seamless PipeAp - FPSOCd - Pitting Corrosion
Cm - Surface Aspect by SEMDf - Corrosion
More from these cases