Crevice Corrosion in a Subsea System — Aspect Before Analysis

Macrography of a ring transverse section presenting a large variation in the grain size, revealing the diferences in the solidification rate.
453
ML00166 / Jul.2020
Tin Bronze Wear Ring of Seawater Pump
M - Tin BronzeP - Wear RingAp - ShipCd - Removed From Service
Cm - FeCl3+HCl+H2O solution Etched MacroDf - Casting Structure
ML00083 / Oct.2017
Steel Back of a Bimetallic Engine Bearing
M - Low Carbon SteelP - Cold FormedAp - ShipCd - Removed From Service
Cm - Nital Etched Micrography by OMDf - Surface Layer