ML00052 / Apr.2017
Cold Cracks in API 5CT L80 Tube Welded to a Structural Part
M
- Low Alloy Steel
P
- Seamless tube
Ap
- Offshore
Cd
- Welding Defect
Cm
- Surface Aspect by SEM
Df
- Heat Affected Zone