Crevice Corrosion in a Subsea System — Aspect Before Analysis

General view of the nodular cast iron crankshaft, 240 mm long, in process of heat treatment.  The main and rod bearings, 54 mm diameter, are heat treated  by localized quenching and tempering.
1018
ML00154 / Jan.2019
High Strength Cast Iron Crankshaft
M - Nodular Cast IronP - CastingAp - EngineCd - Surface treatment
Cm - Aspect Before AnalysisDf - General View
Shaft pinion presenting the bearing surface, with machining markes, from where the thermal spray layer was detached.  The diameter of the 880 mm long shaft in this region is about 75 mm.
426
ML00108 / Dec.2017
Thermal Spray Layer in a Pinion Shaft
M - High Strength Low AlloyP - ShaftAp - EngineCd - Coating Defect
Cm - Aspect Before AnalysisDf - General View

More from these cases

ML00108 — Thermal Spray Layer in a Pinion ShaftM - High Strength Low AlloyP - ShaftAp - EngineCd - Coating Defect
ML00108 / Dec.2017
Thermal Spray Layer in a Pinion Shaft
M - High Strength Low AlloyP - ShaftAp - EngineCd - Coating Defect
Cm - Aspect Before AnalysisDf - Layer Detachment