Rolled Plate

3 cases · 24 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00019 / Apr.2017
Transgranular SCC in Boiler Steam Drum
M - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite
Typical branched stress corrosion cracks in a low carbon steel, ferritic-pertlitic structure. The cracks are filled with corrosion products.
771
ML00018 / Apr.2017
SCC in Boiler Steam Drum
M - Low Carbon SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Branched Cracks
The micrography of the transverse section of the plate, as polished, close to the surface.  The material presents intergranular corrosion and some grains were lost.
1184
ML00015 / Oct.2017
Intergranular Corrosion of 304SS Plate
M - Austenitic Stainless SteelP - Rolled PlateAp - RefineryCd - Intergranular Corrosion
Cm - Micrography by OMDf - Intergranular Corrosion

More from these cases

ML00019 — Transgranular SCC in Boiler Steam DrumM - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
ML00019 / Apr.2017
Transgranular SCC in Boiler Steam Drum
M - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite
ML00019 / Apr.2017
Transgranular SCC in Boiler Steam Drum
M - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Branched Cracks
ML00019 / Apr.2017
Transgranular SCC in Boiler Steam Drum
M - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Transgranular Crack
ML00019 / Apr.2017
Transgranular SCC in Boiler Steam Drum
M - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Transgranular Crack
Micrographic detail of the transgranular stress corrosion cracking.
157
ML00019 / Apr.2017
Transgranular SCC in Boiler Steam Drum
M - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Transgranular Crack
ML00018 — SCC in Boiler Steam DrumM - Low Carbon SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Ferritic perlitic structure of the shell plate.
207
ML00018 / Apr.2017
SCC in Boiler Steam Drum
M - Low Carbon SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite
Micrography of the crack at the internal surface of the steam drum.  The shell plate presents a ferritic perlitic structure.
162
ML00018 / Apr.2017
SCC in Boiler Steam Drum
M - Low Carbon SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Branched Cracks
Micrography of a crack, in a sample as polished, presenting the opened crack.
144
ML00018 / Apr.2017
SCC in Boiler Steam Drum
M - Low Carbon SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Micrography by OMDf - Branched Cracks
Stress corrosion cracks propagating in the ferritic-perlitic structure.
120
ML00018 / Apr.2017
SCC in Boiler Steam Drum
M - Low Carbon SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Branched Cracks
Micrography of a crack, as polished, presenting the cracks filled with corrosion products.
100
ML00018 / Apr.2017
SCC in Boiler Steam Drum
M - Low Carbon SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Micrography by OMDf - Branched Cracks

+2 more from this case →

ML00015 — Intergranular Corrosion of 304SS PlateM - Austenitic Stainless SteelP - Rolled PlateAp - RefineryCd - Intergranular Corrosion
Microstructure of the plate in the center of the ¼” thickness.  Equiaxed austenitic grains with delta ferrite stringers and grain boundary carbide precipitation (sensitization).
303
ML00015 / Oct.2017
Intergranular Corrosion of 304SS Plate
M - Austenitic Stainless SteelP - Rolled PlateAp - RefineryCd - Intergranular Corrosion
Cm - Micrography by OM using A262 Method ADf - Intergranular Precipitation
Microstructure of the plate in the center of the ¼” thickness.  Equiaxed austenitic grains with delta ferrite stringers and grain boundary carbide precipitation (sensitization).
201
ML00015 / Oct.2017
Intergranular Corrosion of 304SS Plate
M - Austenitic Stainless SteelP - Rolled PlateAp - RefineryCd - Intergranular Corrosion
Cm - Micrography by OM using A262 Method ADf - Intergranular Precipitation
Micrographic aspect of a longitudinal section of the plate, close to the surface, in a region where it was detected intergranular corrosion up to 0,5 mm depth.  As polished.
188
ML00015 / Oct.2017
Intergranular Corrosion of 304SS Plate
M - Austenitic Stainless SteelP - Rolled PlateAp - RefineryCd - Intergranular Corrosion
Cm - Micrography by OMDf - Intergranular Corrosion
Micrographic detail of intergranular corrosion, up to 0,5 mm depth.  As polished.
171
ML00015 / Oct.2017
Intergranular Corrosion of 304SS Plate
M - Austenitic Stainless SteelP - Rolled PlateAp - RefineryCd - Intergranular Corrosion
Cm - Micrography by OMDf - Intergranular Corrosion
Micrographic aspect of a longitudinal section of the plate, close to the surface, in a region with intergranular corrosion. Several loose grains were removed, indicating that the structure was embrittled by the intergranular corrosion.
171
ML00015 / Oct.2017
Intergranular Corrosion of 304SS Plate
M - Austenitic Stainless SteelP - Rolled PlateAp - RefineryCd - Intergranular Corrosion
Cm - Micrography by OM using A262 Method ADf - Intergranular Corrosion

+4 more from this case →