Pipe

3 cases · 8 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00153 / Jan.2019
X52 in a Tubular Structure
M - CMn SteelP - Seamless PipeAp - StructureCd - Qualified
Cm - Nital Etched Micrography by SEMDf - Weld Metal
ML00132 / May.2018
Seamless Pipe Overlaid with Alloy 625
M - LAS / Ni AlloyP - Seamless PipeAp - Oil and GasCd - Welding
Cm - Chromic Acid Electrolytic EtchedDf - Weld Metal
ML00072 / Jan.2018
Liquation Cracks in a High Strength Joint
M - Low Alloy Medium Carbon QTP - Longitudinal Seam Welded PipeAp - O&G Well DrillingCd - Welding Defect
Cm - Nital Etched Micrography by OMDf - Weld Metal

More from these cases

ML00153 — X52 in a Tubular StructureM - CMn SteelP - Seamless PipeAp - StructureCd - Qualified
ML00153 / Jan.2019
X52 in a Tubular Structure
M - CMn SteelP - Seamless PipeAp - StructureCd - Qualified
Cm - Nital Etched Micrography by OMDf - Weld Metal
ML00132 — Seamless Pipe Overlaid with Alloy 625M - LAS / Ni AlloyP - Seamless PipeAp - Oil and GasCd - Welding
ML00132 / May.2018
Seamless Pipe Overlaid with Alloy 625
M - LAS / Ni AlloyP - Seamless PipeAp - Oil and GasCd - Welding
Cm - Chromic Acid Electrolytic EtchedDf - Weld Metal
ML00132 / May.2018
Seamless Pipe Overlaid with Alloy 625
M - LAS / Ni AlloyP - Seamless PipeAp - Oil and GasCd - Welding
Cm - Chromic Acid Electrolytic EtchedDf - Weld Metal
ML00072 — Liquation Cracks in a High Strength JointM - Low Alloy Medium Carbon QTP - Longitudinal Seam Welded PipeAp - O&G Well DrillingCd - Welding Defect
ML00072 / Jan.2018
Liquation Cracks in a High Strength Joint
M - Low Alloy Medium Carbon QTP - Longitudinal Seam Welded PipeAp - O&G Well DrillingCd - Welding Defect
Cm - Nital Etched Micrography by OMDf - Weld Metal
ML00072 / Jan.2018
Liquation Cracks in a High Strength Joint
M - Low Alloy Medium Carbon QTP - Longitudinal Seam Welded PipeAp - O&G Well DrillingCd - Welding Defect
Cm - Nital Etched Micrography by OMDf - Weld Metal