Pipe
4 cases · 9 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis
Pipe — sub-branches

ML00112 / Dec.2017
1" XXS Pipe Not Qualified For Low Temp
M - Low Carbon SteelP - Seamless PipeAp - RefineryCd - Not according to spec
Cm - Nital Etched Micrography by OMDf - Close to the External Surface

ML00111 / Dec.2017
3/4" XXS Pipe Not Qualified for Low Temp
M - Low Carbon SteelP - Seamless PipeAp - RefineryCd - Not according to spec
Cm - Nital Etched Micrography by OMDf - Close to the External Surface

ML00097 / Nov.2017
Cast SS Tube Removed From High Temperature Service
M - Heat Resistant SteelP - Centrifugally Cast PipeAp - SiderurgyCd - High Temperature
Cm - As polished micrographyDf - Close to the External Surface

ML00038 / Apr.2017
Cast SS Tube for High Temperature Service
M - Heat Resistant SteelP - Centrifugally Cast PipeAp - SiderurgyCd - Creep
Cm - Glyceregia Etched Micrography by OMDf - Close to the External Surface
More from these cases

ML00112 / Dec.2017
1" XXS Pipe Not Qualified For Low Temp
M - Low Carbon SteelP - Seamless PipeAp - RefineryCd - Not according to spec
Cm - Nital Etched Micrography by OMDf - Close to the External Surface

ML00111 / Dec.2017
3/4" XXS Pipe Not Qualified for Low Temp
M - Low Carbon SteelP - Seamless PipeAp - RefineryCd - Not according to spec
Cm - Nital Etched Micrography by OMDf - Close to the External Surface

ML00097 / Nov.2017
Cast SS Tube Removed From High Temperature Service
M - Heat Resistant SteelP - Centrifugally Cast PipeAp - SiderurgyCd - High Temperature
Cm - As polished micrographyDf - Close to the External Surface

ML00038 / Apr.2017
Cast SS Tube for High Temperature Service
M - Heat Resistant SteelP - Centrifugally Cast PipeAp - SiderurgyCd - Creep
Cm - Micrography by OMDf - Close to the External Surface

ML00038 / Apr.2017
Cast SS Tube for High Temperature Service
M - Heat Resistant SteelP - Centrifugally Cast PipeAp - SiderurgyCd - Creep
Cm - Glyceregia Etched Micrography by OMDf - Close to the External Surface