Alpha
3 cases · 3 images for “fracture”
Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00183 / Dec.2022
Ductile Behavior of an Aluminum Wheel
M - Aluminum Silicon MagnesiumP - CastingAp - AutomotiveCd - Ductile Behavior
Cm - Fractography by SEMDf - Ductile Fracture

ML00179 / Feb.2022
Hydrides in Titanium Weld
M - Unalloyed TitaniumP - In Field WeldAp - Chemical IndustryCd - Hydride Formation
Cm - Fractography by SEMDf - Fracture

ML00176 / Nov.2021
Hydride Formation in a Titanium Blade
M - Unalloyed TitaniumP - BladeAp - Oil and GasCd - Hydride Formation
Cm - Fractography by SEMDf - Fracture