Ferrous Alloys
1 case · 2 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis
Condition: Casting Defect ×Standard: J91540 ×Capture method: Scanning Electron Microscope ×clear all
Ferrous Alloys — sub-branches

ML00017 / Apr.2017
Casting Defect in CA6NM
M - Martensitic Stainless SteelP - Machined PartAp - EnergyCd - Casting Defect
Cm - Micrography by SEMDf - Void
More from these cases

ML00017 / Apr.2017
Casting Defect in CA6NM
M - Martensitic Stainless SteelP - Machined PartAp - EnergyCd - Casting Defect
Cm - Micrography by SEMDf - Void