High Alloy Steel

2 cases · 3 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00174 / Jul.2021
Carburization of a 347 SS Welded Joint
M - Austenitic Stainless SteelP - Fabrication WeldAp - EnergyCd - Carburization
Cm - Oxalic Acid Electrolytic EtchDf - Crack
Micrographic detail of the through wall cracking in the middle of the thickness, showing that the cracking is associated to ferrite network in the (super)duplex microstructure.
128
ML00002 / Jan.2018
Preferential Dissolution and Cracks in SDSS
M - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Cm - Micrography by SEMDf - Crack

More from these cases

ML00002 — Preferential Dissolution and Cracks in SDSSM - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Micrographic detail of the cracking, associated to the ferrite network, that presents both corrosion (preferential dissolution) and fracture (clevage) aspects.
128
ML00002 / Jan.2018
Preferential Dissolution and Cracks in SDSS
M - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Cm - Electrolytic Etch Micrography by SEMDf - Crack