Austenitic Stainless Steel

10 cases · 37 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00168 / Aug.2020
SCC of Austenitic SS Flange Stub End
M - Austenitic Stainless SteelP - Stub EndAp - Chemical IndustryCd - Stress Corrosion
Cm - Oxalic Acid Electrolytic EtchDf - Austenite
ML00167 / Aug.2020
Fatigue of a Flared Tubing Connection
M - Austenitic Stainless SteelP - TubingAp - EngineCd - Mechanical Fatigue
Cm - Oxalic Acid Electrolytic EtchDf - Austenite
ML00160 / Apr.2020
High Temperature Degradation of 310SS
M - Austenitic Stainless SteelP - Rectangular TubeAp - Chemical IndustryCd - Scaling
Cm - Oxalic Acid Electrolytic EtchDf - Austenitic with Secondary Precipitation
Low magnification micrography, by optical microscope, of the longitudinal section of a damaged bolt, in the center of the thickness. The microstructure is austenitic, free from carbides.
100
ML00157 / Feb.2020
Bolts Under Chloride SCC Conditions
M - Austenitic Stainless SteelP - BoltAp - Oil and GasCd - Stress Corrosion
Cm - Oxalic Acid Electrolytic EtchDf - Austenite
Micrography of the case, observed in the center of the thickness, showing an equiaxial granular austenitic microstructure, free from carbides.  The structure is typical of a 316 SS, in a solution annealed condition.
176
ML00122 / Feb.2018
Crevice Corrosion in a Subsea System
M - Austenitic Stainless SteelP - CaseAp - Oil and GasCd - Crevice
Cm - Micrography by OM using A262 Method ADf - Austenite
Micrographic detail of the strain hardened austenitic structure in the longitudinal section of the bolt.
441
ML00101 / Nov.2017
High Strength 316SS Bolt
M - Austenitic Stainless SteelP - BoltAp - SubseaCd - Typical manufacturing
Cm - Micrography by OM using A262 Method ADf - Austenite
Micrographic detail of the strain hardened austenitic structure in the longitudinal section of the bolt.
412
ML00087 / Nov.2017
High Strength Austenitic SS Bolt
M - Austenitic Stainless SteelP - BoltAp - SubseaCd - Typical manufacturing
Cm - Micrography by OM using A262 Method ADf - Austenite
ML00095 / Sep.2017
MIC of a Riser Control Line
M - Austenitic Stainless SteelP - Fabrication WeldAp - Oil and GasCd - Brittle Behavior
Cm - Micrography by OM using A262 Method ADf - Austenite

More from these cases

ML00168 — SCC of Austenitic SS Flange Stub EndM - Austenitic Stainless SteelP - Stub EndAp - Chemical IndustryCd - Stress Corrosion
ML00168 / Aug.2020
SCC of Austenitic SS Flange Stub End
M - Austenitic Stainless SteelP - Stub EndAp - Chemical IndustryCd - Stress Corrosion
Cm - Oxalic Acid Electrolytic EtchDf - Austenite
ML00167 — Fatigue of a Flared Tubing ConnectionM - Austenitic Stainless SteelP - TubingAp - EngineCd - Mechanical Fatigue
ML00167 / Aug.2020
Fatigue of a Flared Tubing Connection
M - Austenitic Stainless SteelP - TubingAp - EngineCd - Mechanical Fatigue
Cm - Oxalic Acid Electrolytic EtchDf - Austenite
ML00160 — High Temperature Degradation of 310SSM - Austenitic Stainless SteelP - Rectangular TubeAp - Chemical IndustryCd - Scaling
ML00160 / Apr.2020
High Temperature Degradation of 310SS
M - Austenitic Stainless SteelP - Rectangular TubeAp - Chemical IndustryCd - Scaling
Cm - Oxalic Acid Electrolytic EtchDf - Austenitic with Secondary Precipitation
ML00160 / Apr.2020
High Temperature Degradation of 310SS
M - Austenitic Stainless SteelP - Rectangular TubeAp - Chemical IndustryCd - Scaling
Cm - Oxalic Acid Electrolytic EtchDf - Austenitic with Secondary Precipitation
ML00160 / Apr.2020
High Temperature Degradation of 310SS
M - Austenitic Stainless SteelP - Rectangular TubeAp - Chemical IndustryCd - Scaling
Cm - Oxalic Acid Electrolytic EtchDf - Secondary Precipitation
ML00160 / Apr.2020
High Temperature Degradation of 310SS
M - Austenitic Stainless SteelP - Rectangular TubeAp - Chemical IndustryCd - Scaling
Cm - Oxalic Acid Electrolytic EtchDf - Intergranular Precipitation
ML00160 / Apr.2020
High Temperature Degradation of 310SS
M - Austenitic Stainless SteelP - Rectangular TubeAp - Chemical IndustryCd - Scaling
Cm - NaOH Electrolytic Etched MicroDf - Austenitic with Secondary Precipitation

+4 more from this case →

ML00157 — Bolts Under Chloride SCC ConditionsM - Austenitic Stainless SteelP - BoltAp - Oil and GasCd - Stress Corrosion
ML00157 / Feb.2020
Bolts Under Chloride SCC Conditions
M - Austenitic Stainless SteelP - BoltAp - Oil and GasCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Strain Hardened
ML00157 / Feb.2020
Bolts Under Chloride SCC Conditions
M - Austenitic Stainless SteelP - BoltAp - Oil and GasCd - Stress Corrosion
Cm - Oxalic Acid Electrolytic EtchDf - Strain Hardened
ML00122 — Crevice Corrosion in a Subsea SystemM - Austenitic Stainless SteelP - CaseAp - Oil and GasCd - Crevice
Micrographic detail of the fully austenitic granular structure of the case, in the center of the thickness.
158
ML00122 / Feb.2018
Crevice Corrosion in a Subsea System
M - Austenitic Stainless SteelP - CaseAp - Oil and GasCd - Crevice
Cm - Micrography by OM using A262 Method ADf - Austenite
ML00101 — High Strength 316SS BoltM - Austenitic Stainless SteelP - BoltAp - SubseaCd - Typical manufacturing
ML00101 / Nov.2017
High Strength 316SS Bolt
M - Austenitic Stainless SteelP - BoltAp - SubseaCd - Typical manufacturing
Cm - Micrography by OM using A262 Method ADf - Strain Hardened
ML00101 / Nov.2017
High Strength 316SS Bolt
M - Austenitic Stainless SteelP - BoltAp - SubseaCd - Typical manufacturing
Cm - Micrography by OM using A262 Method ADf - Strain Hardened
ML00101 / Nov.2017
High Strength 316SS Bolt
M - Austenitic Stainless SteelP - BoltAp - SubseaCd - Typical manufacturing
Cm - Micrography by OM using A262 Method ADf - Strain Hardened
ML00101 / Nov.2017
High Strength 316SS Bolt
M - Austenitic Stainless SteelP - BoltAp - SubseaCd - Typical manufacturing
Cm - Micrography by OM using A262 Method ADf - Strain Hardened
ML00101 / Nov.2017
High Strength 316SS Bolt
M - Austenitic Stainless SteelP - BoltAp - SubseaCd - Typical manufacturing
Cm - Micrography by OM using A262 Method ADf - Austenite
ML00087 — High Strength Austenitic SS BoltM - Austenitic Stainless SteelP - BoltAp - SubseaCd - Typical manufacturing
ML00087 / Nov.2017
High Strength Austenitic SS Bolt
M - Austenitic Stainless SteelP - BoltAp - SubseaCd - Typical manufacturing
Cm - Micrography by OM using A262 Method ADf - Strain Hardened
ML00087 / Nov.2017
High Strength Austenitic SS Bolt
M - Austenitic Stainless SteelP - BoltAp - SubseaCd - Typical manufacturing
Cm - Micrography by OM using A262 Method ADf - Strain Hardened
ML00087 / Nov.2017
High Strength Austenitic SS Bolt
M - Austenitic Stainless SteelP - BoltAp - SubseaCd - Typical manufacturing
Cm - Micrography by OM using A262 Method ADf - Strain Hardened
ML00087 / Nov.2017
High Strength Austenitic SS Bolt
M - Austenitic Stainless SteelP - BoltAp - SubseaCd - Typical manufacturing
Cm - Micrography by OM using A262 Method ADf - Strain Hardened
ML00087 / Nov.2017
High Strength Austenitic SS Bolt
M - Austenitic Stainless SteelP - BoltAp - SubseaCd - Typical manufacturing
Cm - Micrography by OM using A262 Method ADf - Austenite
ML00095 — MIC of a Riser Control LineM - Austenitic Stainless SteelP - Fabrication WeldAp - Oil and GasCd - Brittle Behavior
ML00095 / Sep.2017
MIC of a Riser Control Line
M - Austenitic Stainless SteelP - Fabrication WeldAp - Oil and GasCd - Brittle Behavior
Cm - Micrography by OM using A262 Method ADf - Fusion Line
ML00095 / Sep.2017
MIC of a Riser Control Line
M - Austenitic Stainless SteelP - Fabrication WeldAp - Oil and GasCd - Brittle Behavior
Cm - Micrography by OM using A262 Method ADf - Fusion Line