Chilled Cast Iron

1 case · 2 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00060 / Apr.2017
Brittle Fracture of a Chilled Cast Iron Camshaft
M - Chilled Cast IronP - ShaftAp - AutomotiveCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - In the Center of the Thickness

More from these cases

ML00060 — Brittle Fracture of a Chilled Cast Iron CamshaftM - Chilled Cast IronP - ShaftAp - AutomotiveCd - Brittle Fracture
ML00060 / Apr.2017
Brittle Fracture of a Chilled Cast Iron Camshaft
M - Chilled Cast IronP - ShaftAp - AutomotiveCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - In the Center of the Thickness